Behavior of a superaustenitic stainless steel weld cladding deposited by the gas metal arc welding process

被引:7
|
作者
Matias, Joao V. S. [1 ,4 ]
Lourenco, Manuel J. C. [1 ]
Jorge, Jorge C. F. [1 ]
de Souza, Luis Felipe G. [1 ]
Farneze, Humberto N. [1 ]
Mendes, Matheus C. [1 ]
da Silva, Cilene Labre Alves [2 ]
Araujo, Leonardo S. [3 ]
机构
[1] CEFET RJ, Dept Engn Mecan, Ave Maracana 229, BR-20271110 Rio De Janeiro, RJ, Brazil
[2] CBPF, Ctr Brasileiro Pesquisas Fis, Rio Da Janeiro, Brazil
[3] Univ Fed Rio de Janeiro, Programa Engn Met & Mat, Rio De Janeiro, RJ, Brazil
[4] Inst Fed Fluminense IFF, Lab Ensaios Mat, Cabo Frio, RJ, Brazil
来源
关键词
Superaustenitic steel; Weld metal; GMAW process; Cladding; Microstructure; Corrosion; PITTING CORROSION BEHAVIOR; NI-CR-MO; MECHANICAL-PROPERTIES; AISI; 904L; SIGMA-PHASE; HEAT INPUT; MICROSTRUCTURE; RESISTANCE; PRECIPITATION; DUPLEX;
D O I
10.1016/j.mtcomm.2022.104978
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The performance of a superaustenitic stainless steel weld metal containing 6%Mo deposited by the GMAW process was studied. Multipass welding by the GMAW process with three layers was performed on a carbon steel plate with average heat input of 0.8 kJ/mm. After welding, microstructure characterization by scanning electron microscopy and electron backscattering diffraction, and corrosion performance by cyclic polarization and potentiostatic tests to determine the pitting potential and critical pitting temperature were performed on samples extracted at 3 mm from the fusion line, the minimum thickness required. The weld metal containing 6%Mo showed a microstructure consisting of an austenitic matrix with a volume fraction of Chi and Laves phases inferior to 1% and a PREN value higher than 40 at the dendrite core. As a consequence, similar pitting potential and critical pitting temperature compared to original alloys containing 6%Mo were obtained. Thus, superaustenitic stainless steel weld metals containing 6%Mo have the potential to be suggested as an alternative for weld claddings in the oil and gas industry.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Stainless steel cladding deposited by automatic gas metal arc welding
    Murugan, N
    Parmar, RS
    WELDING JOURNAL, 1997, 76 (10) : S391 - S403
  • [2] Droplet transfer behavior and weld formation of gas metal arc welding for high nitrogen austenitic stainless steel
    Dongqing, Yang
    Hanying, Xiong
    Yong, Huang
    Dejun, Yan
    Dong, Li
    Yong, Peng
    Kehong, Wang
    JOURNAL OF MANUFACTURING PROCESSES, 2021, 65 (65) : 491 - 501
  • [3] Microstructural evolution of superaustenitic stainless steel weld metal subjected to post welding heat treatment
    Jorge, Jorge C. F.
    de Souza, Luis Felipe G.
    Farneze, Humberto N.
    Silva, Cilene L. A.
    Mendes, Matheus C.
    Matias, Joao V. S.
    Araujo, Leonardo S.
    Tavares, Sergio S. M.
    MATERIALS LETTERS, 2023, 344
  • [4] NITROGEN ABSORPTION OF STAINLESS STEEL WELD METAL DURING GAS TUNGSTEN ARC WELDING.
    Kuwana, Takeshi
    Kokawa, Hiroyuki
    Naitoh, Ken-ichiro
    Transactions of the Japan Welding Society, 1986, 17 (02): : 117 - 123
  • [5] Effects of Gas Metal Arc Welding Parameters on Weld Deposit Area of Stainless Steel Claddings
    Kannan, T.
    JOURNAL FOR MANUFACTURING SCIENCE AND PRODUCTION, 2009, 10 (02) : 123 - 135
  • [6] Effect of process parameters on weld quality during double-pulsed gas metal arc welding of dissimilar stainless steel
    Hu Y.
    Xue J.
    Jin L.
    Dong C.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2018, 39 (07): : 115 - 120
  • [7] Study on gas metal arc welding procedure of stainless steel
    Furusawa, Kotokaze
    Yasuda, Kastuhiko
    Yosetsu Gakkai Ronbunshu/Quarterly Journal of the Japan Welding Society, 2000, 18 (01): : 33 - 39
  • [8] Laser welding of superaustenitic stainless steel
    Perricone, MJ
    DuPont, JN
    TRENDS IN WELDING RESEARCH, PROCEEDINGS, 2003, : 47 - 52
  • [9] Evaluation of weld metal hot cracking susceptibility in superaustenitic stainless steel
    Kook-soo Bang
    Seong-hyun Pak
    Sang-kon Ahn
    Metals and Materials International, 2013, 19 : 1267 - 1273
  • [10] Evaluation of weld metal hot cracking susceptibility in superaustenitic stainless steel
    Bang, Kook-soo
    Pak, Seong-hyun
    Ahn, Sang-kon
    METALS AND MATERIALS INTERNATIONAL, 2013, 19 (06) : 1267 - 1273