Investigation of photocatalytic activity (under visible light) of ultrathin CZTS films produced in different thicknesses by PLD method

被引:15
|
作者
Dursun, Sami [1 ]
Sariipek, Fatma Bayram [2 ]
Kilic, Sumeyye [6 ]
Gezgin, Serap Yigit [3 ]
Gundogdu, Yasemin [4 ,5 ]
Kilic, Hamdi Sukur [3 ,5 ]
机构
[1] Konya Tech Univ, Dept Met & Mat Engn, Konya, Turkiye
[2] Konya Tech Univ, Dept Chem Engn, Konya, Turkiye
[3] Selcuk Univ, Fac Sci, Dept Phys, TR-42031 Selcuklu, Konya, Turkiye
[4] Selcuk Univ, Kadinhani Faik Icil Vocat High Sch, Dept Comp Technol, TR-42031 Kadinhani, Konya, Turkiye
[5] Selcuk Univ, Laser Induced Proton Therapy Applicat & Res Ctr, Konya, Turkiye
[6] Selcuk Univ, Dept Met & Mat Engn, Konya, Turkiye
关键词
CZTS-ultrathin film; Thickness; Crystalline; Photocatalysis; Organic dye removel; TIO2; THIN-FILMS; ORGANIC POLLUTANTS; WASTE-WATER; CU2ZNSNS4; NANOCRYSTALS; REMOVAL; DEGRADATION; REMEDIATION; PERFORMANCE; METALS;
D O I
10.1007/s11082-022-04417-w
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Cu2ZnSnS4 (CZTS) thin films in 61 nm, 112 nm, 242 nm and 313 nm thickness which have been produced by Pulsed Laser Deposition (PLD) on Soda Lime Glass substrates as a function of the number of laser pulses. As the deposition of ablated material has been augmented with increasing number of laser pulses, it has been noticed that CZTS-ultrathin film's thicknesses and particle sizes have been increased, their crystalline structures have been improved. Larger particles limit the transmission of light and cause thin films to absorb photons. The band gaps of CZTS (61 nm), CZTS (112 nm), CZTS (242 nm) and CZTS (313 nm) thin film which have been determined to be 1.95 eV, 1.90 eV, 1.50 eV and 1.45 eV, respectively. CZTS (61 nm) ultrathin film with the thinnest one among the thin films produced in this work, which is Cu and S poor but Sn and Zn rich. By increasing the thickness of the film, it has been observed that the amount of Cu and S were increased, and the ratio of Sn and Zn were decreased. In addition, it has been systematically investigated that the photocatalytic activity of the ultra-thin CZTS films coated in different thicknesses by PLD method. Among all the photocatalysts, the CZTS (in 242 nm thickness) photocatalyst has exhibited the highest photocatalytic performance, managing to remove 96.1% of methylene blue (MB) in 240 min. Furthermore, the mechanism that performs photocatalysis has been investigated by scavenger experiments, and it was observed that & BULL;O-2(-) radical ions have an important role in the reaction, while holes have little effect.
引用
收藏
页数:15
相关论文
共 50 条
  • [1] Investigation of photocatalytic activity (under visible light) of ultrathin CZTS films produced in different thicknesses by PLD method
    Sami Dursun
    Fatma Bayram Sarıipek
    Sümeyye Kılıç
    Serap Yiğit Gezgin
    Yasemin Gündoğdu
    Hamdi Şükür Kılıç
    Optical and Quantum Electronics, 2023, 55
  • [2] Photocatalytic activity of molybdenum disulfide nanotube arrays with different wall thicknesses under visible light
    He, Yilin
    Lan, Jinshen
    Qu, Shanzhi
    Ma, Mengwei
    Zheng, Yifan
    Zheng, Xuanli
    Guo, Shengshi
    Huang, Shengli
    Li, Shuping
    Kang, Junyong
    PHYSICS LETTERS A, 2024, 520
  • [3] Polymeric hybrid films with photocatalytic activity under visible light
    Zanrosso, Crissie Dossin
    Piazza, Diego
    Lansarin, Marla Azario
    JOURNAL OF APPLIED POLYMER SCIENCE, 2018, 135 (23)
  • [4] Investigation of the photocatalytic activity of titanium dioxide films under visible light measured by electrospray mass spectrometry
    Souza, Diego H. P.
    Guimaraes, Robson R.
    Correra, Thiago C.
    Zamarion, Vitor M.
    NEW JOURNAL OF CHEMISTRY, 2018, 42 (22) : 18259 - 18268
  • [5] Enhanced visible light photocatalytic activity of bismuth oxybromide lamellas with decreasing lamella thicknesses
    Li, Haiping
    Liu, Jingyi
    Liang, Xuefeng
    Hou, Wanguo
    Tao, Xutang
    JOURNAL OF MATERIALS CHEMISTRY A, 2014, 2 (23) : 8926 - 8932
  • [6] Enhancement of Photocatalytic Performance of Ga2O3 Films with Different Thicknesses Under UVC Light
    Ebru Şenadım Tüzemen
    Catalysis Letters, 2025, 155 (6)
  • [7] Gas Phase Photocatalytic Activity of Ultrathin Pt Layer Coated on α-Fe2O3 Films under Visible Light Illumination
    Zhang, Zhonghai
    Hossain, Md Faruk
    Miyazaki, Takayuki
    Takahashi, Takakazu
    ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2010, 44 (12) : 4741 - 4746
  • [8] Effect of nickel doping on the photocatalytic activity of ZnO thin films under UV and visible light
    Kaneva, Nina V.
    Dimitrov, Dimitre T.
    Dushkin, Ceco D.
    APPLIED SURFACE SCIENCE, 2011, 257 (18) : 8113 - 8120
  • [9] Investigation of the Visible Light-Sensitive ZnO Photocatalytic Thin Films
    Nadareishvili, M.
    Mamniashvili, G.
    Jishiashvili, D.
    Abramishvili, G.
    Ramana, C.
    Ramsden, J.
    ENGINEERING TECHNOLOGY & APPLIED SCIENCE RESEARCH, 2020, 10 (02) : 5524 - 5527
  • [10] Nanocrystalline materials with enhanced photocatalytic activity under visible light
    Cardona-Martinez, Nelson
    Roman, Rafael Mendez
    Rivera, Sindia
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2006, 231