Heat treatment response of additively manufactured 17-4PH stainless steel

被引:25
|
作者
Lashgari, H. R. [1 ,2 ,3 ]
Adabifiroozjaei, E. [2 ,3 ]
Kong, C. [4 ]
Molina-Luna, Leopoldo [2 ,3 ]
Li, S. [1 ]
机构
[1] Univ New South Wales, Sch Mat Sci & Engn, Sydney, NSW 2052, Australia
[2] ALS Ind, Asset Integr & Reliabil Dept, Sydney, NSW 2164, Australia
[3] Tech Univ Darmstadt, Dept Mat & Geosci, Alarich Weiss Str 2, D-64287 Darmstadt, Germany
[4] Univ New South Wales, Mark Wainwright Analyt Ctr MWAC, Sydney, NSW 2052, Australia
关键词
Solution treatment; 17-4PH stainless steel; Reversed austenite; Tensile strength; Hardness; MECHANICAL-PROPERTIES; AUSTENITE; TRANSFORMATION; PRECIPITATION; EVOLUTION;
D O I
10.1016/j.matchar.2023.112661
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Unlike conventional 17-4PH stainless steels where thermal treatment (solution annealing + aging) leads to X95% martensite and X5% retained austenite, additively manufactured 17-4PH stainless steels are not responsive to conventional thermal treatment and considerable fraction of retained and/or reversed austenite is formed during solution treatment and aging. In the present study, we have investigated how applying various thermal treatments (i.e., solutionising within the temperature range of 1040 degrees C-1240 degrees C from 0.25 h to 4 h and aging at temperature of 480 degrees C from 1 h to 8 h) affect the microstructure, volume fraction of retained/reversed austenite, hardness, and tensile properties of thermally treated 17-4PH stainless steel manufactured by selective laser melting (SLM) process. For comparison, additively manufactured parts were subject to direct aging without initial solution treatment. The results showed the occurrence of significant partitioning of Ni and Cu in reversed austenite as both elements are strong FCC stabilizer. The presence of inclusions inherent from powder metallurgy (SiO2 and MnS) acts as high-energy interface promoting the heterogenous nucleation of reversed austenite. The results showed that direct aging without initial solution treatment continuously decreased the volume fraction of retained austenite which can be related to the precipitation of Cu-rich precipitates and change in chemical stability of the austenite. It was observed that in the solutionised sample at 1040 degrees C, the volume fraction of retained austenite increased with solution time at the beginning and reached a maximum value of X44% after 1 h and then it decreased to X11.5% after 4 h. However, this trend was not the case for the solutionised samples at 1240 degrees C. The increase of solution temperature from 1040 degrees C to 1240 degrees C resulted in decreasing the volume fraction of retained austenite to less than X5%. The distribution and enrichment of Ni and Cu in the austenite affecting the chemical stability of austenite and presence of inclusions are major factors controlling the volume fraction of retained/reversed austenite at different thermal treatment conditions. The lowest amount of austenite (X4.3%) was measured in the solutionised alloy at 1240 degrees C-4 h followed by aging at 480 degrees C for 1 h. Direct aging at 480 degrees C for 3 h increased the hardness by X45% and further increase of aging time to 8 h decreased the hardness. For solutionised samples, conventional solution treatment at 1040 degrees C regardless of solution treatment time (0.25 h to 4 h) did not result in peak hardness during aging due to the considerable volume fraction of retained and/or reversed austenite and low diffusivity of Cu in the austenite. The ultimate tensile strength (UTS) of the solutionised sample at 1240 degrees C-4 h followed by aging at 480 degrees C-1 h (UTS X1227 MPa) and directly aged sample at 480 degrees C-3 h (UTS X1211 MPa) without initial solution treating were found to be X30% higher than that of as-printed alloy (UTS X945 MPa) due to the presence of least amount of austenite in the matrix (X5-8%).
引用
收藏
页数:17
相关论文
共 50 条
  • [1] Optimization of Aging Temperature and Heat-Treatment Pathways in Additively Manufactured 17-4PH Stainless Steel
    Chae, Hobyung
    Lim, Sangyeob
    Lee, Taeho
    Shin, Eunjoo
    Suh, Joowon
    Kang, Suk Hoon
    Lee, Soo Yeol
    MATERIALS, 2023, 16 (24)
  • [2] Dynamic Constitutive Behavior of Additively Manufactured 17-4PH Stainless Steel
    Fox, C.
    Tilton, C.
    Rousseau, C-E
    Shukla, A.
    Sheeley, C.
    Hebert, R.
    JOURNAL OF DYNAMIC BEHAVIOR OF MATERIALS, 2022, 8 (02) : 242 - 254
  • [3] Dynamic Constitutive Behavior of Additively Manufactured 17-4PH Stainless Steel
    C. Fox
    C. Tilton
    C-E. Rousseau
    A. Shukla
    C. Sheeley
    R. Hebert
    Journal of Dynamic Behavior of Materials, 2022, 8 : 242 - 254
  • [4] Rotary friction welding of additively manufactured 17-4PH stainless steel
    Lashgari, H. R.
    Li, S.
    Kong, C.
    Asnavandi, M.
    Zangeneh, Sh
    JOURNAL OF MANUFACTURING PROCESSES, 2021, 64 : 1517 - 1528
  • [5] Effect of heat treatments on microstructural evolution of additively manufactured and wrought 17-4PH stainless steel
    Sun, Yu
    Hebert, Rainer J.
    Aindow, Mark
    MATERIALS & DESIGN, 2018, 156 : 429 - 440
  • [6] Microstructural characterization and mechanical properties of additively manufactured 17-4PH stainless steel
    Eskandari, H.
    Lashgari, H. R.
    Ye, L.
    Eizadjou, M.
    Wang, H.
    MATERIALS TODAY COMMUNICATIONS, 2022, 30
  • [7] Impact of composition on the heat treatment response of additively manufactured 17-4 PH grade stainless steel
    Meredith, S. D.
    Zuback, J. S.
    Keist, J. S.
    Palmer, T. A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 738 : 44 - 56
  • [8] Fatigue Testing of Additively Manufactured 17-4PH Stainless Steel Samples with a Stress Concentration
    Coatney, Michael D.
    Lawrence, Bradley D.
    Henry, Todd C.
    Nataraj, Latha
    Hubbard, Clifford
    FRACTURE, FATIGUE, FAILURE AND DAMAGE EVOLUTION, VOL 3, 2023, : 53 - 60
  • [9] On mesoscale strain fluctuations in tensile tests on additively manufactured 17-4PH stainless steel
    Bouaziz, Mohamed Ali
    Djouda, Joseph Marae
    Hild, Francois
    JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN, 2022, 57 (08): : 688 - 701
  • [10] Comparing Stress Corrosion Cracking Behavior of Additively Manufactured and Wrought 17-4PH Stainless Steel
    Shoemaker, Trevor K.
    Harris, Zachary D.
    Burns, James T.
    CORROSION, 2022, 78 (06) : 528 - 546