The optimal high-temperature piezoelectric cuts of α-BiB3O6 crystals and their fatigue behaviors at high-temperature and low-pressure

被引:1
|
作者
Xu, Mengyan [1 ]
Ma, Zhihong [1 ]
Wang, Guoliang [1 ]
Peng, Xiangkang [1 ]
Liu, Zijian [1 ]
Liu, Wei [1 ]
Zhao, Xian [1 ]
Yu, Fapeng [1 ]
机构
[1] Shandong Univ, Ctr Opt Res & Engn, State Key Lab Crystal Mat, Jinan 250100, Peoples R China
基金
中国国家自然科学基金;
关键词
ELECTROELASTIC PROPERTIES; ELASTIC PROPERTIES; SINGLE-CRYSTAL; GROWTH; DEPENDENCE; FEATURES;
D O I
10.1039/d3ce01317k
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
High-temperature piezoelectric materials with good temperature stability are essential for various sensors fabrication. The monoclinic piezoelectric crystals alpha-BiB3O6 (BIBO) not only possess high resistivity, but also strong piezoelectric behaviors, and are promising for high-temperature sensing application. In this study, the temperature stability of electro-elastic coefficients of BIBO crystals was studied by using an impedance method. Results reveal that the piezoelectric coefficients d(21) and d(22) exhibited excellent temperature stability over the tested temperature range of 20-650 degrees C, and the variations were found to be <+/- 5%. In addition, the optimal sensitive cuts relevant to the longitudinal extensional vibration mode (LE), face shear vibration mode (FS) and thickness shear vibration mode (TS) were designed, and the maximum piezoelectric coefficients values for the LE, FS and TS modes were 40.0, -20.6 and 37.8 pC N-1, respectively. Furthermore, the fatigue behaviors of the BIBO crystal cuts annealed at high-temperature of 650 degrees C and low-pressure of 5 x 10(-3) Pa for 10-20 h were investigated, where the dielectric and piezoelectric properties were showing a slight decrease, relating to the formation of oxygen vacancies, as confirmed by the electron paramagnetic resonance (EPR) spectra. In total, the BIBO crystals obtained show stable piezoelectric behaviors with neglegible attenuation (<5%) after annealing treatment, indicating its merits for piezoelectric sensing over a wide temperature range under low-pressure environments.
引用
收藏
页码:1556 / 1564
页数:9
相关论文
共 50 条
  • [1] High-performance, high-temperature piezoelectric BiB3O6 crystals
    Yu, Fapeng
    Lu, Qingming
    Zhang, Shujun
    Wang, Hewei
    Cheng, Xiufeng
    Zhao, Xian
    JOURNAL OF MATERIALS CHEMISTRY C, 2015, 3 (02) : 329 - 338
  • [2] Investigation of a BiB3O6 crystal growth mechanism by high-temperature Raman spectroscopy
    Wan, Songming
    Teng, Bing
    Zhang, Xia
    You, Jinglin
    Zhou, Wenping
    Zhang, Qingli
    Yin, Shaotang
    CRYSTENGCOMM, 2010, 12 (01): : 211 - 215
  • [3] STABILITY OF ORTHOENSTATITE AT HIGH-TEMPERATURE AND LOW-PRESSURE
    CARLSON, WD
    SWINNEA, JS
    MISER, DE
    AMERICAN MINERALOGIST, 1988, 73 (11-12) : 1255 - 1263
  • [4] High-temperature piezoelectric crystals and devices
    Holger Fritze
    Journal of Electroceramics, 2011, 26 : 122 - 161
  • [5] High-temperature piezoelectric crystals and devices
    Fritze, Holger
    JOURNAL OF ELECTROCERAMICS, 2011, 26 (1-4) : 122 - 161
  • [6] LOW-CYCLE HIGH-TEMPERATURE FATIGUE OF SOME HIGH-TEMPERATURE ALLOYS
    JAYARAMAN, N
    GADEMSKY, P
    LERCH, B
    ROMANOSKI, GR
    ANTOLOVICH, SD
    JOURNAL OF METALS, 1980, 32 (08): : 77 - 77
  • [7] Diffusion in High-temperature Piezoelectric Single Crystals
    Sauerwald, J.
    Schulz, M.
    Richter, D.
    Fritze, H.
    HIGH TEMPERATURE CORROSION AND MATERIALS CHEMISTRY 8, 2010, 25 (25): : 135 - 146
  • [8] Stability and Applications of High-Temperature Piezoelectric Crystals
    Fritze, H.
    Schulz, M.
    Richter, D.
    2014 IEEE INTERNATIONAL CONFERENCE ON OXIDE MATERIALS FOR ELECTRONIC ENGINEERING (OMEE), 2014, : 219 - 220
  • [9] High-temperature low-pressure chemical vapor deposition of β-Ga2O3
    Zhang, Yuxuan
    Feng, Zixuan
    Karim, Md Rezaul
    Zhao, Hongping
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2020, 38 (05):
  • [10] THERMAL MODELING IN LOW-PRESSURE HIGH-TEMPERATURE METAMORPHIC BELTS
    DEYOREO, JJ
    LUX, DR
    GUIDOTTI, CV
    TECTONOPHYSICS, 1991, 188 (3-4) : 209 - 238