An experimental and numerical study of spatial and temporal catalyst degradation during start-up and shut-down of PEM fuel cells

被引:3
|
作者
Hou, Yuze [1 ]
Schall, Johannes [1 ]
Dietze, Steve [1 ]
Kurz, Timo [1 ]
Gerteisen, Dietmar [1 ]
机构
[1] Fraunhofer Inst Solar Energy Syst ISE, Freiburg, Germany
关键词
Degradation; Start -up shut-down; Segmented fuel cell; Numerical modeling; PEM fuel cell; CARBON CORROSION; 3D MODEL; OPERATION; FLOW;
D O I
10.1016/j.jpowsour.2023.233780
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Degradation during start-up and shut-down (SUSD) of proton exchange membrane (PEM) fuel cells is investigated both experimentally and numerically. In order to understand spatial degradation, the local cell voltage and electrochemical surface area (ECSA) during SUSD are measured using a segmented cell. Novel phenomena such as undegraded inlet segments and a gradual rise in resting potential at the start of the test are hence observed. To further interpret the experimental data, an advanced SUSD model is developed, which accurately reproduces detailed experimental phenomena. The local potential is calculated independently based on the mixture gas concentration and kinetics, without imposing an artificial hydrogen/air interface, allowing for a more realistic transition of the membrane phase potential. The study shows that hydrogen has a greater influence on local membrane phase potential than air due to its faster reaction kinetics and residual hydrogen in inlet gas during SD can safeguard the inlet segments against degradation.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Selective anode catalyst for the mitigation of start-up/shut-down induced cathode degradation in proton exchange membrane fuel cells
    Stuehmeier, Bjoern M.
    Damjanovic, Ana Marija
    Rodewald, Katia
    Gasteiger, Hubert A.
    JOURNAL OF POWER SOURCES, 2023, 558
  • [2] ANALYSES OF THE START-UP AND SHUT-DOWN OF SCWR FUEL QUALIFICATION TEST LOOP
    Vojacek, Ales
    Mazzini, Guido
    PROCEEDINGS OF THE 22ND INTERNATIONAL CONFERENCE ON NUCLEAR ENGINEERING - 2014, VOL 2B, 2014,
  • [3] Cathode catalyst layer aging of proton exchange membrane fuel cell during emulated start-up/shut-down phases
    Drugeot, Timothee
    Wane, Raky
    Micoud, Fabrice
    Pinton, Eric
    Guetaz, Laure
    Mermoux, Michel
    Bultel, Yann
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 87 : 838 - 847
  • [4] Quantitative analysis of carbon corrosion during fuel cell start-up and shut-down by anode purging
    Linse, Nicolas
    Scherer, Guenther G.
    Wokaun, Alexander
    Gubler, Lorenz
    JOURNAL OF POWER SOURCES, 2012, 219 : 240 - 248
  • [5] Start-up and shut-down fluidized bed combustion boilers
    Wiese, D.
    Gericke, B.
    VGB-Kraftwerkstechnik, 1987, 67 (12): : 1147 - 1158
  • [6] Degradation Study by Start-Up/Shut-Down Cycling of Superhydrophobic Electrosprayed Catalyst Layers Using a Localized Reference Electrode Technique
    Ferreira-Aparicio, Paloma
    Chaparro, Antonio M.
    Antonia Folgado, M.
    Conde, Julio J.
    Brightman, Edward
    Hinds, Gareth
    ACS APPLIED MATERIALS & INTERFACES, 2017, 9 (12) : 10626 - 10636
  • [7] SMOOTHING START-UP AND SHUT-DOWN COSTS - CONCAVE CASE
    SOBEL, MJ
    MANAGEMENT SCIENCE SERIES A-THEORY, 1970, 17 (01): : 78 - 91
  • [8] SMOOTHING START-UP AND SHUT-DOWN COSTS IN SEQUENTIAL PRODUCTION
    SOBEL, MJ
    OPERATIONS RESEARCH, 1969, 17 (01) : 133 - &
  • [9] Experimental assessment of proton exchange membrane fuel cell performance degradations during emulated start-up/shut-down phases
    Drugeot, Timothee
    Micoud, Fabrice
    Pinton, Eric
    Rosini, Sebastien
    Poirot-Crouvezier, Jean-Philippe
    Poupin, Lucas
    Bultel, Yann
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2023, 48 (14) : 5630 - 5642
  • [10] Oxygen Evolution Co-Catalysts at Fuel Cell Cathodes for Degradation Mitigation during Simulated Start-up Shut-down Cycles
    Srivastava, Ratndeep
    Strasser, Peter
    PROTON EXCHANGE MEMBRANE FUEL CELLS 9, 2009, 25 (01): : 565 - 571