Investigation on Thermal Barrier Coating Damages for Ultrafast Laser Drilling of Cooling Holes

被引:2
|
作者
Wang, Shaojian [1 ]
Hu, Yue [1 ]
Zuo, Yangjie [1 ]
Yang, Zenan [2 ]
Jiang, Ruisong [1 ]
机构
[1] Sichuan Univ, Sch Aeronaut & Astronaut, Chengdu 610200, Peoples R China
[2] Beijing Inst Aeronaut Mat, Sci & Technol Adv High Temp Struct Mat Lab, Beijing 100095, Peoples R China
关键词
picosecond laser; thermal barrier coating microholes; processing quality;
D O I
10.3390/ma16155395
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
To mitigate the challenges pertaining to coating damage and processing defects arising from the utilization of ultrafast laser drilling for microhole creation in thermal barrier coatings (TBCs), thereby exerting substantial influence on the long-term durability of these microholes, the investigation proposes a comprehensive methodology. It encompasses the design of a two-factor four-level full factorial experiment and the execution of experimental research on picosecond laser drilling of TBC microholes. By meticulously analyzing the morphology of the microholes and the coating interface, the damage mechanisms associated with picosecond laser drilling of TBC microholes, as well as the influence of laser process parameters on coating damage, are revealed. The findings reveal that the optimal microhole entrance quality and the lowest roughness along the hole perimeter are attained at a laser power of 12 W and a scanning speed of 320 mm/s. Moreover, at a laser power of 30 W and a scanning speed of 320 mm/s, the minimal crack length on the blunt angle side of the hole and the highest machining quality are observed.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Laser drilling of cooling holes through plasma sprayed thermal barrier coatings
    Voisey, KT
    Clyne, TW
    SURFACE & COATINGS TECHNOLOGY, 2004, 176 (03): : 296 - 306
  • [2] Evaluation of laser drilling of holes in thermal barrier coated superalloys
    Bathe, R.
    Padmanabham, G.
    MATERIALS SCIENCE AND TECHNOLOGY, 2014, 30 (14) : 1778 - 1782
  • [3] Femtosecond Laser Micro Drilling of Cooling Holes on Thermal Barrier Coated Titanium Alloy for Aeroengine Application
    Deepu, P.
    Jagadesh, T.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (19) : 10242 - 10263
  • [4] Film Cooling With a Thermal Barrier Coating: Round Holes, Craters, and Trenches
    Davidson, F. Todd
    KistenMacher, David A.
    Bogard, David G.
    JOURNAL OF TURBOMACHINERY-TRANSACTIONS OF THE ASME, 2014, 136 (04):
  • [5] FILM COOLING WITH A THERMAL BARRIER COATING: ROUND HOLES, CRATERS AND TRENCHES
    Davidson, F. Todd
    Kistenmacher, David A.
    Bogard, David G.
    PROCEEDINGS OF THE ASME TURBO EXPO 2012, VOL 4, PTS A AND B, 2012, : 1757 - 1768
  • [6] Numerical investigation on laser stripping of thermal barrier coating
    Marimuthu, S.
    Kamara, A. M.
    Sezer, H. K.
    Li, L.
    Ng, G. K. L.
    COMPUTATIONAL MATERIALS SCIENCE, 2014, 88 : 131 - 138
  • [7] Crack behavior in ultrafast laser drilling of thermal barrier coated nickel superalloy
    Zheng, Changlong
    Zhao, Kai
    Shen, Hong
    Zhao, Xiaofeng
    Yao, Zhenqiang
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2020, 282
  • [8] Investigation on millijoule femtosecond laser spiral drilling of micro-deep holes in thermal barrier coated alloys
    Rujia Wang
    Xia Dong
    Kedian Wang
    Xiaomao Sun
    Zhengjie Fan
    Wenqiang Duan
    The International Journal of Advanced Manufacturing Technology, 2021, 114 : 857 - 869
  • [9] Investigation on millijoule femtosecond laser spiral drilling of micro-deep holes in thermal barrier coated alloys
    Wang, Rujia
    Dong, Xia
    Wang, Kedian
    Sun, Xiaomao
    Fan, Zhengjie
    Duan, Wenqiang
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 114 (3-4): : 857 - 869
  • [10] Interfacial Stresses of Thermal Barrier Coating with Film Cooling Holes Induced by CMAS Infiltration
    Chiu, Chenchun
    Tseng, Shaochen
    Chao, Chingkong
    Fan, Xueling
    Cheng, Weihung
    COATINGS, 2022, 12 (03)