The Effects of Oscillating Frequency on Microstructure and Hardness of W-Ni-Fe Refractory Alloy Sintered by Hot Oscillating Pressure

被引:1
|
作者
Gao, Ka [1 ]
Hu, Yanghu [2 ]
Zhang, Zixiang [1 ]
Ren, Chunyang [1 ]
Zhao, Wei [3 ]
Sun, Dejian [4 ]
Gao, Yang [4 ]
An, Linan [5 ]
Kong, Qingquan [6 ]
机构
[1] Univ Shanghai Sci & Technol, Sch Mech Engn, Shanghai 200093, Peoples R China
[2] China Natl Heavy Machinery Res Inst Co Ltd, State Key Lab Met Extrus & Forging Equipment Techn, Xian 710000, Peoples R China
[3] Changhai Hosp, Dept Gen Med, Shanghai 200000, Peoples R China
[4] Zhengzhou Univ Aeronaut, Sch Mat Sci & Engn, Zhengzhou 450015, Peoples R China
[5] Dongguan Univ Technol, Sch Mech Engn, Dongguan 523808, Peoples R China
[6] Chengdu Univ, Sichuan Prov Engn Technol Res Ctr Powder Met, Chengdu 610106, Peoples R China
基金
中国国家自然科学基金;
关键词
hardness; hot oscillating pressure; microstructure; oscillating frequency; W-Ni-Fe alloy; MECHANICAL-PROPERTIES; HEAVY ALLOYS; TUNGSTEN; DENSIFICATION; TEMPERATURE;
D O I
10.1002/adem.202301326
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
90 W-7Ni-3Fe refractory alloys are first sintered by hot oscillating pressure (HOP) under different oscillating frequencies (0, 1, and 10 Hz) in this work. The effects of oscillating frequencies on the microstructure and Vickers hardness are investigated. With the oscillating frequency increasing, the relative density and hardness of refractory alloys are obviously improved. Especially, the alloy sintered at the oscillating frequency of 10 Hz had the highest relative density of approximately 98.9% and the smallest average grain size of 3.26 mu m. Moreover, the narrowest average thickness of the bonding phase is about 0.18 mu m, and the lowest tungsten contiguity is about 61.1%. Then its excellent hardness (456.8 HV30) is obtained, which is nearly 16.1% higher than that of the 0 Hz frequency alloy. The refractory alloy with high densification, small grain size, and good hardness could be obtained by HOP with a high oscillating frequency. W-Ni-Fe refractory alloy is prepared by hot oscillating pressure at different oscillating frequencies (0, 1, and 10 Hz). The higher relative density (98.9%) and excellent hardness (456.8 HV30) of sintered alloys with the narrowest average thickness bonding phase (0.18 mu m), lowest tungsten contiguity (61.1%), and smallest grain size (3.26 mu m) are significantly improved through higher oscillating frequency applied.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:6
相关论文
共 50 条
  • [1] W-Ni-Fe Refractory Alloy Sintered by Hot Oscillating Pressure Under Different Amplitudes
    Gao, Ka
    Zhao, Junliang
    Sun, Dejian
    Gao, Yang
    An, Linan
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (12)
  • [2] Oscillating pressure sintering of W-Ni-Fe refractory alloy
    Gao, Ka
    Xu, Yueyang
    Tang, Gaopeng
    Fan, Lei
    Zhang, Rui
    An, Linan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 805 (789-793) : 789 - 793
  • [3] Oscillating pressure sintered W-Cu refractory alloy with high density and hardness under lower temperature
    Gao, Ka
    Liu, Dongyue
    Ma, Tianyu
    Zhao, Junliang
    Sun, Dejian
    Gao, Yang
    Pan, Kunming
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2022, 102
  • [4] Hot oscillatory pressure sintered W-Ni-Fe refractory alloy under different sintering pressures: Microstructures, densification behavior and properties
    Gao, Ka
    Zhao, Junliang
    Zhao, Wei
    Ren, Chunyang
    Kong, Qingquan
    Duan, Zhenxia
    An, Linan
    VACUUM, 2023, 214
  • [5] PRECIPITATION IN A LIQUID-PHASE SINTERED W-NI-FE ALLOY
    MUDDLE, BC
    EDMONDS, DV
    ACTA METALLURGICA, 1985, 33 (12): : 2119 - 2128
  • [6] Effect of heat treatment temperature on the microstructure and hardness of AlCoCrNiFe high-entropy alloy sintered by hot oscillating pressing
    Gao, Ka
    Hu, Yanghu
    Zhang, Zixiang
    Ren, Chunyang
    Xiong, Yan
    Sun, Dejian
    Gao, Yang
    KOVOVE MATERIALY-METALLIC MATERIALS, 2024, 62 (05): : 267 - 273
  • [7] The effect of managanese addition on the microstructure of W-Ni-Fe heavy alloy
    Eun-Pyo Kim
    Moon-Hee Hong
    Woon Hyung Baek
    In-Hyung Moon
    Metallurgical and Materials Transactions A, 1999, 30 : 627 - 632
  • [8] The effect of manganese addition on the microstructure of W-Ni-Fe heavy alloy
    Kim, EP
    Hong, MH
    Baek, WH
    Moon, IH
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (03): : 627 - 632
  • [9] Microstructure and properties of AlCoCrNiFe high-entropy alloy sintered by hot oscillating pressing
    Gao, Ka
    Liu, Dongyue
    Sun, Dejian
    Gao, Yang
    Wang, Zhaohui
    An, Linan
    INTERMETALLICS, 2023, 154
  • [10] Effect of Ta addition on the sinterability of spark plasma sintered W-Ni-Fe alloy
    Muthuchamy, A.
    Srikanth, Muthe
    Yadav, Dig Vijay
    Annamalai, A. Raja
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2023, 237 (10) : 1518 - 1525