Microstructural characterization of AM60-TixNby nanocomposite powders processed by high-energy ball milling

被引:3
|
作者
Abbas, Aqeel [1 ]
Hussein, M. A. [1 ]
Javid, Mohamed [2 ]
机构
[1] King Fahd Univ Petr & Minerals KFUPM, Interdisciplinary Res Ctr Adv Mat, Dhahran 31261, Saudi Arabia
[2] King Fahd Univ Petr & Minerals, Core Res Facil, Dhahran 31261, Saudi Arabia
关键词
Mg composite; Nanocrystalline composite; AM60; High energy ball milling; LATTICE STRUCTURE EVOLUTION; TI COMPOSITE POWDERS; MECHANICAL-PROPERTIES; CORROSION BEHAVIORS; MAGNESIUM ALLOY; MG; AL; NI; METALLURGY; STRENGTH;
D O I
10.1016/j.matchemphys.2023.128718
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Magnesium alloys are one of the lightest metal alloys and are considered potential candidates for structural and hydrogen storage applications. High-energy ball milling is an efficient powder metallurgy technique to produce fine composite particles. The AM60 Magnesium alloy was ball milled with different reinforcement concentrations (5Nb,10Nb, 5Ti,10Ti, 3Ti+7Nb, and 3Nb+7Ti) wt% for 10 h and 20 h. The morphology and microstructure were analyzed using a scanning electron microscope equipped with energy dispersive spectrometry and field emission transmission electron microscope. The crystallite size, lattice strain, and solid solubility were analyzed using XRD. It was observed that higher milling time has refined the particle size. The XRD analysis revealed that a maximum crystallite size of 17 nm was observed in the AM60Ti10 composite after 10 h and a minimum of 14 nm in the AM60Ti3Nb7 composite after 20 h milling time. The results revealed that niobium and titanium reduced the crystallite size and enhanced the lattice strain synergistically. The maximum lattice strain (0.066 %) and dislocation density (9 nm-2) were observed in the AM60Nb7Ti3 composite after 20 h milling time. The SEM results revealed The AM60Nb10 composite after 20 h presents a minimum particle size of (9 mu m), while AM60Ti5 has a maximum particle size of 15 mu m after 10 h milling. The Ti addition causes agglomeration and the AM60Ti5 composite has the maximum average particle size of 15 mu m after 10 h milling. The SEM results revealed that flattened agglomerates are formed as the result of higher milling energy during the collision.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Characterization of titanium powders processed in n-hexane by high-energy ball milling
    Restrepo, A. H.
    Rios, J. M.
    Arango, F.
    Correa, E.
    Zuleta, A. A.
    Valencia-Escobar, A.
    Bolivar, F. J.
    Castano, J. G.
    Echeverria, F. E.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2020, 110 (7-8): : 1681 - 1690
  • [2] Characterization of titanium powders processed in n-hexane by high-energy ball milling
    A. H. Restrepo
    J. M. Ríos
    F. Arango
    E. Correa
    A. A. Zuleta
    A. Valencia-Escobar
    F. J. Bolivar
    J. G Castaño
    F. E. Echeverría
    The International Journal of Advanced Manufacturing Technology, 2020, 110 : 1681 - 1690
  • [3] Effect of Ball Size on the Microstructure and Morphology of Mg Powders Processed by High-Energy Ball Milling
    Rios, Jesus
    Restrepo, Alex
    Zuleta, Alejandro
    Bolivar, Francisco
    Castano, Juan
    Correa, Esteban
    Echeverria, Felix
    METALS, 2021, 11 (10)
  • [4] Characterization of the structure of TiB2/TiC nanocomposite powders fabricated by high-energy ball milling
    Wang, Huihua
    Wu, Wenyuan
    Sun, Shucheng
    Bian, Xue
    Tu, Ganfeng
    CERAMICS INTERNATIONAL, 2011, 37 (07) : 2689 - 2693
  • [5] High-energy ball milling and characterization of Al-Si alloy powders
    School of Materials Science and Engineering, Central South University, Changsha 410083, China
    Zhongnan Daxue Xuebao (Ziran Kexue Ban), 2008, 1 (29-34):
  • [6] Microstructural characterization of nanocrystalline SiC synthesized by high-energy ball-milling
    Ghosh, B.
    Pradhan, S. K.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 486 (1-2) : 480 - 485
  • [7] Microstructural characterization of Mg-SiC nanocomposite synthesized by high energy ball milling
    Kamrani, S.
    Penther, D.
    Ghasemi, A.
    Riedel, R.
    Fleck, C.
    ADVANCED POWDER TECHNOLOGY, 2018, 29 (07) : 1742 - 1748
  • [8] Microstructural characterization of amorphous and nanocrystalline boron nitride prepared by high-energy ball milling
    Ghosh, J.
    Mazumdar, S.
    Das, M.
    Ghatak, S.
    Basu, A. K.
    MATERIALS RESEARCH BULLETIN, 2008, 43 (04) : 1023 - 1031
  • [9] Microstructural Characterization of Mg-SiC Nanocomposite Powders Fabricated by High Energy Mechanical Milling
    Bemanifar, Saeed
    Rajabi, Mohammad
    Hosseinipour, Seyed Jamal
    SILICON, 2017, 9 (06) : 823 - 827
  • [10] Microstructural Characterization of Mg-SiC Nanocomposite Powders Fabricated by High Energy Mechanical Milling
    Saeed Bemanifar
    Mohammad Rajabi
    Seyed Jamal Hosseinipour
    Silicon, 2017, 9 : 823 - 827