Thermal shock resistance and crack growth behavior of Aurivillius phase Bi4Ti3O12-based ferroelectric ceramics

被引:0
|
作者
Qian Xu [1 ]
Shaoxiong Xie [1 ]
Yu Chen [2 ,3 ]
Qingyuan Wang [1 ,2 ]
机构
[1] MOE Key Laboratory of Deep Earth Science and Engineering, College of Architecture and Environment, Sichuan University
[2] School of Mechanical Engineering, Chengdu University
[3] College of Materials Science and Engineering, Sichuan University
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
D O I
暂无
中图分类号
TQ174.1 [基础理论];
学科分类号
0805 ; 080502 ;
摘要
A type of W/Cr co-doped Bi4Ti3O12(ab. BTWC) ceramics were synthesized utilizing the traditional solid-state reaction process, and its thermal shock resistance(TSR) as well as the crack growth behavior was systematically investigated by water quenching technology. It can be found by the succeeded fractographic analysis that many edge thermal cracks began to appear in the samples subjected to thermal shock with ΔT=400°C. According to an integrated TSR model, the critical thermal-shock temperature difference ΔTCwas calculated to be 356°C. Moreover, it can be noticed that the indenter induced crack growth behaviors under thermal shock loads presented three stages, i.e. no growth, large growth, and moderate growth, along with ΔT increasing from 0°C to 700°C. Finally, the asymmetry of P-E hysteresis loops was observed and understood by the orientated polarization of defect dipoles after the sample was thermally shocked, while the water-quenching process above the Curie temperature of the ceramics could lead to a random orientation of the defect dipoles. This research can not only evaluate the service conditions of Bi4Ti3O12high-temperature piezoceramics, but also understand the failure mechanism of bismuth layer structured ferroelectric ceramics in the case of thermal shock.
引用
收藏
页码:248 / 254
页数:7
相关论文
共 50 条
  • [1] Thermal shock resistance and crack growth behavior of Aurivillius phase Bi4Ti3O12-based ferroelectric ceramics
    Xu, Qian
    Xie, Shaoxiong
    Chen, Yu
    Wang, Qingyuan
    PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2021, 31 (02) : 248 - 254
  • [2] Aurivillius ceramics:: Bi4Ti3O12-based piezoelectrics
    Jardiel, T.
    Caballero, A. C.
    Villegas, M.
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2008, 116 (1352) : 511 - 518
  • [3] Bi4Ti3O12-Based Ferroelectric Ceramics Designed for Extreme Conditions
    Marakhovskiy M.A.
    Talanov M.V.
    Panich A.A.
    Bulletin of the Russian Academy of Sciences: Physics, 2023, 87 (09) : 1317 - 1321
  • [4] Differences in nature of electrical conductions among Bi4Ti3O12-based ferroelectric polycrystalline ceramics
    Long, Changbai
    Chang, Qi
    Fan, Huiqing
    SCIENTIFIC REPORTS, 2017, 7
  • [5] Differences in nature of electrical conductions among Bi4Ti3O12-based ferroelectric polycrystalline ceramics
    Changbai Long
    Qi Chang
    Huiqing Fan
    Scientific Reports, 7
  • [6] Enhanced piezoelectric properties and temperature stability of Bi4Ti3O12-based Aurivillius ceramics via W/Nb substitution
    Xie, Xinchun
    Wang, Tianzi
    Zhou, Zhiyong
    Cheng, Guofeng
    Liang, Ruihong
    Dong, Xianlin
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (04) : 957 - 962
  • [7] High oxide ion conductivity in layer-structured Bi4Ti3O12-based ferroelectric ceramics
    Long, Changbai
    Ren, Wei
    Li, Yiwen
    Liu, Laijun
    Xia, Yuanhua
    Fan, Huiqing
    JOURNAL OF MATERIALS CHEMISTRY C, 2019, 7 (29) : 8825 - 8835
  • [8] POLARIZATION BEHAVIOR OF FERROELECTRIC BI4TI3O12 CERAMICS
    JOVALEKIC, C
    PAVLOVIC, M
    OSMOKROVIC, P
    ZDUJIC, M
    IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 1995, 2 (03) : 409 - 412
  • [9] Polarization behavior of ferroelectric Bi4Ti3O12ceramics
    Jovalekic, C.
    Pavlovic, M.
    Osmokrovic, P.
    Zdujic, M.
    IEEE, Piscataway (02):
  • [10] Bi4Ti3O12-based lead-free piezoelectric ceramics with grain orientation
    Nagata, H
    Fujita, Y
    Enosawa, H
    Takenaka, T
    ISAF 2002: PROCEEDINGS OF THE 13TH IEEE INTERNATIONAL SYMPOSIUM ON APPLICATIONS OF FERROELECTRICS, 2002, : 303 - 306