Superhydrophobic anti-icing/de-icing SR/CNTs surfaces hot-embossed with femtosecond laser machined mold

被引:0
|
作者
Jiang, Guo [2 ]
He, Binbo [2 ]
Yang, Can [1 ]
机构
[1] Shenzhen Technol Univ, Sinogerman Coll Intelligent Mfg, Shenzhen 518118, Guangdong, Peoples R China
[2] South China Univ Technol, Sch Mech & Automot Engn, Guangzhou, Peoples R China
基金
中国国家自然科学基金;
关键词
femtosecond laser; peak-ridge structures; superhydrophobic; anti-icing; de-icing; FABRICATION; CORROSION; ICE; NANOPARTICLES; ALUMINUM; DESIGN; ROBUST; STEEL;
D O I
10.1177/02670844241283972
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Anti-icing/de-icing surfaces are dispensable in reducing accidents and economic losses caused by accumulated ice and frost on outdoor facilities in cold and humid environments. In this work, a low-cost, reproducible process was presented to fabricate superhydrophobic anti-icing/de-icing surfaces. For this purpose, concave micro-structures were firstly created on the mold steel surface using femtosecond laser machining, and then the corresponding convex micro-structures were prepared on the surface of a silicone rubber (SR) composite mixed with multi-wall carbon nanotubes (CNTs) using hot embossing. Thanks to the presence of unique micro-scale peak-ridge structures, the as-prepared SR/CNTs surfaces possess superhydrophobic characteristic. Long icing delay time was endowed by the large volume of air pockets inside micro-structures, and the icing time was significantly extended from 67 to 416 s, which is ascribed to the greatly inhibited heat transfer between the droplet and the surface. Moreover, the SR/CNTs surface had excellent photothermal conversion capability with the presence of photothermal particles CNTs, and the temperature of the surface increased rapidly from 21.6 to 86.1 degrees C in 5 min under a standard sunlight irradiation. In addition, the SR/CNTs surface also possesses superior photothermal defrosting and de-icing performance as the ice and frost on the surface can be quickly melted under a standard sunlight intensity irradiation and the de-icing rate is up to 0.92 mg/s. Finally, the good reusability of the mold steel and the resistance to mechanical wear and chemical corrosion of superhydrophobic SR/CNTs surface found in this work make the proposed approach promising for industrial mass production and anti-icing/de-icing applications in harsh environments.
引用
收藏
页码:895 / 906
页数:12
相关论文
共 50 条
  • [1] Fabrication of anti-icing/de-icing surfaces by femtosecond laser
    Tang, Bo-Hao
    Wang, Qiang
    Han, Xing-Chen
    Zhou, Hao
    Yan, Xiao-Jing
    Yu, Yi
    Han, Dong-Dong
    FRONTIERS IN CHEMISTRY, 2022, 10
  • [2] Research and application of anti-icing and de-icing on superhydrophobic surfaces
    Wang, Yubo
    Sun, Yongyang
    Xue, Yiqing
    Liang, Wenyan
    Harbin Gongcheng Daxue Xuebao/Journal of Harbin Engineering University, 2024, 45 (08): : 1497 - 1507
  • [3] Superhydrophobic and Photothermal PVDF/CNTs Durable Composite Coatings for Passive Anti-Icing/Active De-Icing
    Jiang, Guo
    Liu, Zhongyang
    Hu, Jinhuan
    ADVANCED MATERIALS INTERFACES, 2022, 9 (02):
  • [4] A photothermal and superhydrophobic emulsified asphalt coating modified by CNTs and PTFE for anti-icing and de-icing applications
    Peng, Chao
    Yang, Dongjin
    You, Zhanping
    Ruan, Di
    Guan, Peiwen
    Ye, Zhile
    Ning, Yunfei
    Zhao, Ni
    Yang, Feiyu
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 416
  • [5] Superhydrophobic-electrothermal laser-induced graphene for effectively anti-icing and de-icing
    Niu, Yifan
    Sun, Yuekun
    Tao, Xingfu
    Liao, Chenxi
    Yao, Jiawei
    COMPOSITES COMMUNICATIONS, 2024, 46
  • [6] Robust photothermal superhydrophobic concrete coating for efficient anti-icing/de-icing
    Zhang, Ning
    Kong, Xiangqing
    Chang, Yahui
    Qiao, Wanfu
    Zhang, Mingliang
    Kang, Ran
    JOURNAL OF BUILDING ENGINEERING, 2025, 101
  • [7] Research progress on application of superhydrophobic materials in anti-icing and de-icing technology
    Li J.
    Jiao W.
    Wang Y.
    Yin Y.
    Chu Z.
    He X.
    Fuhe Cailiao Xuebao/Acta Materiae Compositae Sinica, 2022, 39 (01): : 23 - 38
  • [8] Femtosecond laser fabrication of superhydrophobic metallic surfaces with anti-icing properties
    Volpe, Annalisa
    Di Venere, Leonardo
    Gaudiuso, Caterina
    Licciulli, Francesco
    Giordano, Francesco
    Ancona, Antonio
    LASER-BASED MICRO- AND NANOPROCESSING XV, 2021, 11674
  • [9] Aircraft anti-icing and de-icing techniques and modeling
    Thomas, SK
    Cassoni, RP
    MacArthur, CD
    JOURNAL OF AIRCRAFT, 1996, 33 (05): : 841 - 854
  • [10] Anti-icing and de-icing methods used for icing at wings of aircrafts
    Akgun, Osman
    Kalayci Doner, Nimeti
    JOURNAL OF POLYTECHNIC-POLITEKNIK DERGISI, 2024,