Strength and Porosity of Special Coke Used in Electrothermal Processes

被引:0
|
作者
Ulyeva, G. A. [1 ]
机构
[1] Qarmet, Analyt Monitoring Ctr, Temirtau, Kazakhstan
关键词
special-purpose coke; porosity; rexil; Shubarkol coal; long-flame coal; industrial-grade silicon; electrothermal production; SILICON PRODUCTION;
D O I
10.3103/S1068364X24600891
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The mechanical strength and pore structure of special-purpose coke are determined in classical and thermooxidative coking (heating rate 2.3 and >30 degrees C/min, respectively). The relationship between the coke's strength and porosity is established. By mercury porosimetry, the volume of the pores and their distribution within the coke are determined. In the thermooxidative coking of long-flame Shubarkol coal, the pore size of the special-purpose coke obtained (800-1200 nm) is an order of magnitude greater than that of regular coke (100 nm).