Corrosion of pure Ni and two Ni-based alloys in presence of ZnCl2-KCl salt deposit

被引:0
|
作者
Li, Y.S.
Wang, F.G.
Niu, Y.
Wu, W.T.
机构
来源
| 2001年 / Rare Metals Materials and Engineering Press卷 / 30期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
相关论文
共 50 条
  • [1] Corrosion of pure Ni and two Ni-based alloys in presence of ZnCl2-KCl salt deposit
    Li, YS
    Wang, FG
    Niu, Y
    Wu, WT
    RARE METAL MATERIALS AND ENGINEERING, 2001, 30 (05) : 376 - 379
  • [2] Accelerated corrosion of pure Fe, Ni, Cr and several Fe-based alloys induced by ZnCl2-KCl at 450°C in oxidizing environment
    Li, YS
    Niu, Y
    Wu, WT
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 345 (1-2): : 64 - 71
  • [3] Corrosion of pure Fe and 310SS beneath ZnCl2-KCl salt film at 450 °C
    Li, Yuanshi
    Niu, Yan
    Liu, Gang
    Wu, Weitao
    1600, Chinese Academy of Sciences (36):
  • [4] Effect of salt deposit on corrosion behavior of Ni-based alloys and stainless steels in supercritical water
    Yang, Jianqiao
    Wang, Shuzhong
    Li, Yanhui
    Tang, Xingying
    Wang, Yuzhen
    Xu, Donghai
    Guo, Yang
    JOURNAL OF SUPERCRITICAL FLUIDS, 2019, 152
  • [5] Corrosion behavior of 316SS and Ni-based alloys in a ternary NaCl-KCl-MgCl2 molten salt
    Sun, Hua
    Wang, Jianqiang
    Li, Zhijun
    Zhang, Peng
    Su, Xingzhi
    SOLAR ENERGY, 2018, 171 : 320 - 329
  • [6] 纯Ni和Ni基合金在ZnCl2-KCl盐膜下的腐蚀
    李远士
    王富岗
    朱焱
    吴维
    稀有金属材料与工程, 2001, (05) : 376 - 379
  • [7] Effects of alloying elements on the corrosion behavior of Ni-based alloys in molten NaCl-KCl-MgCl2 salt at different temperatures
    Sun, Hua
    Zhang, Peng
    Wang, Jianqiang
    CORROSION SCIENCE, 2018, 143 : 187 - 199
  • [8] Effects of alloying elements (Mo and W) on corrosion behavior of Ni-based alloys in NaCl-KCl-MgCl2 2 molten salt
    Chi, Liangdao
    Sun, Hua
    Zhou, Xingtai
    CORROSION SCIENCE, 2024, 237
  • [9] Electrochemical-Impedance-Spectroscopy Study of Corrosion of Fe and Ni with Molten ZnCl2-KCl Coating in Air at 673K
    Pan, T. J.
    Lin, Y. F.
    Hu, J.
    Zeng, C. L.
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2009, 28 (04) : 233 - 244
  • [10] Corrosion of pure iron and two commercial steels beneath ZnCl2-Kcl deposits in a controlled atmosphere containing HCl at 500 °C
    Zhang, K
    Niu, Y
    Wu, WT
    ACTA METALLURGICA SINICA, 2004, 40 (04) : 388 - 392