Creep behavior and damage feature of Re/Ru-containing single crystal nickel-based superalloy at high temperature

被引:0
|
作者
Yan H.-J. [1 ,2 ]
Tian S.-G. [2 ]
Dong Z.-F. [1 ]
Zhao G.-Q. [2 ]
Tian N. [2 ]
Zhang S.-K. [2 ]
机构
[1] School of Mechanical Electronic & Information Engineering, China University of Mining & Technology, Beijing
[2] School of Mechanical Engineering, Guizhou University of Engineering Science, Bijie
关键词
Creep damage; Deformation mechanism; Microstructure; Re/Ru; Single crystal nickel-based superalloy;
D O I
10.11817/j.ysxb.1004.0609.2021-37713
中图分类号
学科分类号
摘要
The creep behavior and damage feature of a 4.5%Re/3%Ru-containing single crystal nickel-based superalloy at high temperature were investigated of creep property measurement and microstructure observation. The results show that the creep life of alloy at (1100 ℃, 140 MPa) is measured as 476 h. During steady state creep at high temperature, the deformation mechanism of alloy is dislocation slipping in γ matrix and climbing over the rafted γ' phase. In the later stage of creep, the deformation mechanism of alloy is dislocations slipping in γ matrix and shearing into the rafted γ' phase. Wherein the dislocations shearing into γ' phase can cross-slip from {111} to {100} planes to form the configuration of K-W locking + APB, which may improve the creep resistance of alloy. The alternated slipping of a large number of 〈110〉 dislocations causes both the twisting and breaking of the rafted γ/γ' phases and the crystal rotation of γ' phase to form the sub-grain structure, which may reduce the creep resistance of alloy. Furthermore, the alternated activation of the initiation/secondary slipping systems may promote the initiation of cracks occurring in the rafted γ/γ' interface, and the cracks are propagated along the interface perpendicular to the stress axis until creep fracture, which is the damage and fracture mechanism of alloy in the later stage creep at high temperature. © 2021, Science Press. All right reserved.
引用
收藏
页码:401 / 409
页数:8
相关论文
共 24 条
  • [1] FUCHS G E., Solution heat treatment response of a third generation single crystal Ni-base superalloy, Materials Science and Engineering A, 300, 1, pp. 52-60, (2001)
  • [2] CUI Ren-jie, HUANG Zhao-hui, Microstructual evolution and stability of second generation single crystal nickel-based superalloy DD5, Transactions of Nonferrous Metals Society of China, 26, 8, pp. 2079-2085, (2016)
  • [3] SUN Xiao-feng, JIN Tao, ZHOU Yi-wei, Et al., Research progress of nickel base single crystal superalloy, Materials China, 31, 12, pp. 1-11, (2012)
  • [4] XIANG J Y, XIE F Q, WU X Q, Et al., Study on development trend of superalloy in China based on patent analysis, Materials Review, 28, 2, pp. 100-106, (2014)
  • [5] GUO J T, ZHOU L Z, YUAN C, Et al., Microstructure and properties of several originally invented and unique superalloys in China, Transactions of Nonferrous Metals Society of China, 21, 2, pp. 237-249, (2011)
  • [6] WANG Xiao-meng, WANG Tian-you, ZHAO Zi-hua, Et al., Effect of creep damage behavior and solution treatment on properties of turbine blades, Journal of Aeronautics, 35, 10, pp. 2784-2793, (2014)
  • [7] HEMKER K J, MILLS M J, NIX W D., An investigation of the mechanisms that control intermediate temperature creep of Ni<sub>3</sub>Al, Acta Metallurgica et Materialia, 39, 8, pp. 1901-1913, (1991)
  • [8] ZHANG J X, WANG J C, HARADA H, Et al., The effect of lattice misfit on the dislocation motion in superalloys during high-temperature low-stress creep, Acta Materialia, 53, 17, pp. 4623-4633, (2005)
  • [9] TIAN S G, ZHANG B S, SHU D L, Et al., Creep properties and deformation mechanism of the containing 4.5Re/3.0Ru single crystal nickel-based superalloy at high temperatures, Materials Science and Engineering A, 643, pp. 119-126, (2015)
  • [10] HECKL A, NEUMEIER S, GOKEN M., The effect of Re and Ru on γ/γ' microstructure, γ-solid solution strengthening and creep strength in nickel-base superalloys, Materials Science and Engineering A, 528, pp. 3435-3444, (2011)