A comparative investigation on the surface characteristics of AISI 304 and AISI 1045 steel influenced by turning combined with ball burnishing

被引:0
|
作者
Raza, Ahmed [1 ]
Kumar, Sudhanshu [1 ]
机构
[1] Maulana Azad Natl Inst Technol, Dept Mech Engn, Bhopal 462003, MP, India
关键词
Burnishing tool; surface roughness; hardness; specific wear rate; corrosion resistance; 1045; steels; 304; RESISTANCE ENHANCEMENT; CORROSION-RESISTANCE; MAGNESIUM ALLOY; RESIDUAL-STRESS; TITANIUM-ALLOY; ROUGHNESS; TI-6A1-4V; BEHAVIOR;
D O I
10.1177/14644207241263793
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Burnishing is a popular superfinishing procedure in the manufacturing industry that induces plastic deformation to the finished product by the application of a highly polished and hardened deforming element known as a burnishing tool. Research work on the burnishing process is numerous. However, the reports containing the comparative investigations are lacking. In this work, the effect of ball burnishing parameters namely penetration depth, burnishing spindle speed, and number of passes has been compared and analyzed on AISI 1045 and AISI 304 steels with respect to surface roughness, hardness, wear resistance, and corrosion resistance. Results indicate that the combination of a feed rate of 0.12 mm/rev, spindle speed of 160 rpm, and penetration depth of 0.025 mm with four passes generated minimum surface roughness (AISI 1045). However, maximum surface hardness is obtained with a feed rate of 0.12 mm/rev, spindle speed of 160 rpm, and at 0.085 mm penetration depth under one pass (AISI 304). The lowest specific wear rate is achieved with a feed rate of 0.12 mm/rev at a spindle speed of 160 rpm and a penetration depth of 0.085 mm in one pass (AISI 304). The burnishing process influenced both materials, AISI 304 and AISI 1045, under varying parametric conditions. The maximum reduction in surface roughness is 68.1% for AISI 304 and 79.3% for AISI 1045, while surface hardness improves by 27% for AISI 304 and 22% for AISI 1045. Additionally, the burnishing process reduces the specific wear rate by 49.3% for AISI 304 and 45.4% for AISI 1045. The refinement of grains during the burnishing process enhances corrosion resistance compared to the unburnished surface.
引用
收藏
页码:335 / 352
页数:18
相关论文
共 50 条
  • [1] AN INVESTIGATION INTO THE BALL BURNISHING OF AN AISI-1045 FREE-FORM SURFACE
    LEE, SSG
    TAM, SC
    LOH, NH
    MIYAZAWA, S
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1992, 29 (1-3) : 203 - 211
  • [2] Influence of mechanical (ball burnishing) surface treatment on fatigue behaviour of AISI 1045 steel
    Sadeler, R.
    Akbulut, M.
    Atasoy, S.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2013, 51 (01): : 31 - 35
  • [3] Roller burnishing on 1045AISI steel
    Diaz, Silvio
    Robert, Teresita
    CIENCIA E INGENIERIA, 2007, 28 (02): : 75 - 81
  • [4] Ultrasonic-assisted ball burnishing of aluminum 6061 and AISI 1045 steel
    Amini, Saeid
    Bagheri, Alireza
    Teimouri, Reza
    MATERIALS AND MANUFACTURING PROCESSES, 2018, 33 (11) : 1250 - 1259
  • [5] Influence of ball-burnishing on roughness, hardness and corrosion resistance of AISI 1045 steel
    Saldana-Robles, Alberto
    Plascencia-Mora, Hector
    Aguilera-Gomez, Eduardo
    Saldana-Robles, Adriana
    Marquez-Herrera, Alfredo
    Angel Diosdado-De la Pena, Jose
    SURFACE & COATINGS TECHNOLOGY, 2018, 339 : 191 - 198
  • [6] Improvement of Surface Quality of AISI 1010 Steel Plates by Ball Burnishing
    Gharbi, F.
    Al-Fadhalah, K. J.
    Tharwan, M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (19) : 10035 - 10047
  • [7] Study of surface quality after turning of steel AISI 304
    Technical University of Košice, Faculty of Manufacturing Technologies, Bayerova 1, Prešov
    080 01, Slovakia
    Manuf. Technol., 4 (527-532):
  • [8] TURNING OF AISI 304 AUSTENITIC STAINLESS STEEL
    Ozek, Cebeli
    Hascalik, Ahmet
    Caydas, Ulas
    Karaca, Faruk
    Unal, Engin
    SIGMA JOURNAL OF ENGINEERING AND NATURAL SCIENCES-SIGMA MUHENDISLIK VE FEN BILIMLERI DERGISI, 2006, 24 (02): : 117 - 121
  • [9] Effect of Roller Burnishing and Slide Roller Burnishing on Fatigue Strength of AISI 304 Steel: Comparative Analysis
    Duncheva, Galya
    Maximov, Jordan
    Anchev, Angel
    Dunchev, Vladimir
    Anastasov, Kalin
    Argirov, Yaroslav
    METALS, 2024, 14 (06)
  • [10] Tool Wear Effect on Surface Integrity in AISI 1045 Steel Dry Turning
    Magalhaes, Laurence Colares
    Carlesso, Gabriel Catarino
    Lopez de Lacalle, Luis Norberto
    Souza, Marcelo Tramontin
    Palheta, Fabiana de Oliveira
    Binder, Cristiano
    MATERIALS, 2022, 15 (06)