Restraint of intermetallic compound and improvement of mechanical performance of Ti/Al dissimilar alloy by rotary friction welding based on laser powder bed fusion

被引:3
|
作者
Hu, Maohui [1 ]
Zhi, Shengxing [2 ]
Chen, Jibing [1 ]
Li, Ruidi [2 ]
Liu, Bowen [1 ]
He, Liang [3 ,4 ]
Yang, Huihui [5 ]
Wang, Hongze [5 ]
机构
[1] Wuhan Polytech Univ, Sch Mech Engn, Wuhan 430023, Peoples R China
[2] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
[3] Sichuan Univ, Sch Mech Engn, State Key Lab Intelligent Construct & Hlth Operat, Chengdu 610065, Peoples R China
[4] Sichuan Univ, West China Hosp, Med X Ctr Mfg, Chengdu 610041, Sichuan, Peoples R China
[5] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Shanghai 200240, Peoples R China
关键词
Dissimilar alloy; Laser powder bed fusion; Rotary friction welding; Microstructure; Intermetallic compound; Mechanical performance; MICROSTRUCTURAL CHARACTERIZATION; WELDED ALUMINUM; JOINT STRENGTH; TITANIUM; INTERFACE; PARAMETERS; TI6AL4V;
D O I
10.1016/j.jmapro.2024.09.021
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Due to titanium and aluminum alloys having the characteristics of low mass density and high specific strength, the welding of both has a unique advantage in the aerospace field. However, traditional friction welding is mainly used for casting and forging materials, and there are few studies on friction welding between Ti and Al alloys fabricated by laser powder bed fusion (L-PBF). Because L-PBF is a kind of rapid solidification methods, the microstructure evolution in rotary friction welding joints should be further studied. In this study, L-PBF was used to prepare Ti6Al4V and AlSi10Mg samples, and rotary friction welding (RFW) was used to prepare rod-shaped welding samples. OM, SEM, and XRD were employed to study the morphology and microstructure of the welding interface, and EDS was used to study the intermetallic compounds (IMCs) of the welding interface. Finally, the microhardness and other mechanical performance of the solder joints were investigated, and the optimal process parameters were obtained. The results showed that the interface grain size of the welded sample prepared by L-PBF and RFW is small, and the IMC produced is TiAl and TiAl3. It is found that the diffusion of AlTi elements is hindered by Si enrichment. When the ratio between friction to forging force of welded specimens was less than 2, the maximum tensile strength could reach 278 MPa, a 50 % improvement over using RFW directly. Moreover, SEM and EDS characterization results showed that the fracture mode of the welded end face was a typical brittle fracture, and the IMC was significantly reduced. This is because the formation of the Si particle networks at the interface inhibits the mutual diffusion of Ti and Al, and the microhardness increases. Therefore, in this research, L-PBF and RFW are combined to produce Ti-Al alloy with high mechanical performance, which provides a feasible strategy for welding dissimilar materials.
引用
收藏
页码:440 / 454
页数:15
相关论文
共 50 条
  • [1] Fabrication of Ti3Al-Based Intermetallic Alloy by Laser Powder Bed Fusion Using a Powder Mixture
    Li, Kuanhe
    Wang, Xianglong
    Chen, Haishao
    Huang, Xiaoxiao
    Zhu, Guanglin
    Tu, Ganfeng
    MATERIALS, 2023, 16 (07)
  • [2] Laser powder bed fusion of a Ni3Al-based intermetallic alloy with tailored microstructure and superior mechanical performance
    Liu, Mingyu
    Wang, Jiang
    Hu, Tao
    Xu, Songzhe
    Shuai, Sansan
    Xuan, Weidong
    Yin, Shuo
    Chen, Chaoyue
    Ren, Zhongming
    ADVANCED POWDER MATERIALS, 2024, 3 (01):
  • [3] Improvement in tensile strength of Mg/Al alloy dissimilar friction stir welding joints by reducing intermetallic compounds
    Chen, Wei
    Wang, Wenxian
    Liu, Zepeng
    Zhai, Xin
    Bian, Gongbo
    Zhang, Tingting
    Dong, Peng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 861
  • [4] Experimental and numerical research on formation mechanism of intermetallic compounds in laser brazing welding for Ti/Al dissimilar alloy
    Zhao, Jintian
    Geng, Shaoning
    Jiang, Ping
    Song, Minjie
    Xu, Boan
    Luo, Qianni
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 : 2930 - 2944
  • [5] Microstructure and Mechanical Properties of a Novel Al-Mg-Sc-Ti Alloy Fabricated by Laser Powder Bed Fusion
    Shu, Zhiheng
    Liu, Yunzhong
    MATERIALS, 2024, 17 (03)
  • [6] Effect of Intermetallic Compound Content on the Laser Welding Performance of Al-Fe Alloy Sheets
    Zhao Pizhi
    Pan Yanfeng
    Jiang Tao
    Shi Xiangjun
    Zhang Qi
    ALUMINIUM ALLOYS 2014 - ICAA14, 2014, 794-796 : 401 - +
  • [7] Development of Al-Ti-based alloys for laser powder bed fusion
    Roscher, M.
    Balachandran, S.
    Mayweg, D.
    Jaegle, E.
    ADDITIVE MANUFACTURING, 2021, 47
  • [8] Microstructure and Mechanical Properties of Dissimilar Friction Welding Ti-6Al-4V Alloy to Nitinol
    Rehman, Ateekh Ur
    Babu, Nagumothu Kishore
    Talari, Mahesh Kumar
    Usmani, Yusuf Siraj
    Al-Khalefah, Hisham
    METALS, 2021, 11 (01) : 1 - 11
  • [9] Effect of Ti microalloying and laser remelting on the microstructure and mechanical properties of laser powder bed fusion Al-12Si alloy
    Hou, Ruosong
    Chen, Jianhao
    Ren, Xuepeng
    Zhao, Yang
    Ding, Yufeng
    Yu, Zunyue
    Ren, Shubin
    Qu, Xuanhui
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 901
  • [10] Influence of Powder Bed Temperature on the Microstructure and Mechanical Properties of Ti-6Al-4V Alloy Fabricated via Laser Powder Bed Fusion
    Xing, Lei-Lei
    Zhang, Wen-Jing
    Zhao, Cong-Cong
    Gao, Wen-Qiang
    Shen, Zhi-Jian
    Liu, Wei
    MATERIALS, 2021, 14 (09)