Friction stir welding of constrained groove pressed Al1050 using Al2O3 nanoparticles

被引:0
|
作者
Keshavarz, Hossein [1 ]
Moosavi, Seyyed Ezzatollah [1 ]
Kazeminezhad, Mohsen [1 ]
Movahedi, Mojtaba [1 ]
机构
[1] Sharif Univ Technol, Dept Mat Sci & Engn, Azadi Ave, Tehran, Iran
关键词
Friction stir welding; Constrained groove pressing; Aluminum; Mechanical properties; Al2O3; MECHANICAL-PROPERTIES; DYNAMIC RECRYSTALLIZATION; ALUMINUM; MICROSTRUCTURE; NANOCOMPOSITES; STRENGTH; BEHAVIOR; JOINT;
D O I
10.1016/j.jmrt.2024.07.198
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this investigation, two passes Constrained Groove Pressed (CGPed) Al1050 sheets went through Friction Stir Welding (FSW) by adding nano-sized Al2O3 particles. Then, the microstructure and mechanical properties of the welded joints, undergone various pass numbers and rotational to traverse speed (w/v) ratios, were presented. Findings showed all joints were fractured from the SZ, although HAZ softening happened due to grain growth in this region. The presence of the Al2O3 particles in the stir zone led to a fine and equiaxed grain structure, resulting from continuous dynamic recrystallization (CDRX) during the high-temperature welding process. This grain refinement contributed to an improvement in the mechanical properties of the joints, such as strength and microhardness. Employing two different w/v ratios resulted in a variety of thermal cycles during the welding procedure such that the peak temperature in the w/v of 70 and 25 r/mm reached 423 degrees C and 285 degrees C, respectively. Microstructure studies via optical observation and EBSD analysis illustrated that employing a higher w/v ratio and weld pass number resulted in more uniform particle distribution in the stir zone thanks to facilitating materials flow and incorporation during FSW. As a result, the three passes FSWed sample at the higher w/v ratio of 70 r/mm showed the most homogeneous particle distribution and finest grain structure in the SZ. This microstructure evolution was in reliable agreement with the mechanical performance of the joints. The three passes FSWed sample at the higher w/v ratio of 70 r/mm demonstrated the highest weld strength, microhardness, and %elongation compared to other FSWed joints. This sample showed an ultimate tensile strength (UTS) of 97 MPa and a %elongation of 16%, and its mean microhardness value had a 3.5% increase compared to the CGPed base metal. Conversely, the one pass FSWed sample at the lower w/v ratio of 25 r/mm represented the weakest mechanical properties due to cavities, defects, and agglomerated Al2O3 nanoparticles. The presence of nanoparticles was a decisive factor in microstructural evolution during the welding, thereby increasing the mechanical quality of the joints dependent upon their uniform dispersion, obtained by increasing the pass number and w/v ratio.
引用
收藏
页码:597 / 608
页数:12
相关论文
共 50 条
  • [1] Friction stir welding of Al2O3 particulate 6061 Al alloy composite
    Nakata, K
    Inoki, S
    Nagano, Y
    Ushio, M
    THERMEC'2003, PTS 1-5, 2003, 426-4 : 2873 - 2878
  • [2] Metallization of Al2O3 ceramic with Mg by friction stir spot welding
    Sonomura, Hirosuke
    Ozaki, Tomoatsu
    Katagiri, Kazuaki
    Hasegawa, Yasunori
    Tanaka, Tsutomu
    Kakitsuji, Atsushi
    CERAMICS INTERNATIONAL, 2021, 47 (09) : 12789 - 12794
  • [3] Friction Stir Welding of AA6082 Thin Aluminium Alloy Reinforced with Al2O3 Nanoparticles
    Mohammed, Sameer
    Birru, Anil Kumar
    TRANSACTIONS OF THE INDIAN CERAMIC SOCIETY, 2019, 78 (03) : 137 - 145
  • [4] Friction Stir Welding of aluminium based composites reinforced with Al2O3 particles
    Ceschini, L.
    Boromei, I.
    Gambaro, C.
    Minak, G.
    Morri, A.
    Tarterini, F.
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 87 - +
  • [5] Microstructure and mechanical characteristics of Al1050/B2O3+Cu hybrid surface nanocomposite fabricated using friction stir processing
    Pedrammehr, Siamak
    Sajed, Moosa
    Pakzad, Sajjad
    Jond, Ahad Zare
    Ettefagh, Mir Mohammad
    Tutunchilar, Saman
    MATERIALS RESEARCH EXPRESS, 2024, 11 (09)
  • [6] Evaluation of microstructure and mechanical properties of Al1050/Al2O3/Gr composite processed by forming operation ECAP
    Hassan, Alhassan Mohammed
    Gattmah, Jabbar
    Shihab, Suha K.
    OPEN ENGINEERING, 2024, 14 (01):
  • [7] Laser butt joining of Al2O3 ceramic plates metallized by friction stir welding
    Sonomura, Hirosuke
    Katagiri, Kazuaki
    Yamaguchi, Takuto
    Tanaka, Keigo
    Ozaki, Tomoatsu
    Hasegawa, Yasunori
    Tanaka, Tsutomu
    Kakitsuji, Atsushi
    CERAMICS INTERNATIONAL, 2022, 48 (16) : 23381 - 23386
  • [8] Microstructural Aspects of the Fabrication of Al/Al2O3 Composite by Friction Stir Processing
    Malopheyev, Sergey S.
    Zuiko, Ivan S.
    Mironov, Sergey Yu.
    Kaibyshev, Rustam O.
    MATERIALS, 2023, 16 (07)
  • [9] Fabrication of Al5083 surface hybrid nanocomposite reinforced by CNTs and Al2O3 nanoparticles using friction stir processing
    Ostovan, Farhad
    Amanollah, Sattar
    Toozandehjani, Meysam
    Shafiei, Ehsan
    JOURNAL OF COMPOSITE MATERIALS, 2020, 54 (08) : 1107 - 1117
  • [10] The optimization of the groove depth height in friction stir welding of AA 6061-T6 with Al2O3 powder particle reinforcement
    Rahul Kesharwani
    Kishor Kumar Jha
    Murshid Imam
    Chiranjit Sarkar
    Journal of Materials Research, 2022, 37 : 3743 - 3760