Improved high-voltage cycling stability of single-crystalline LiNi0.8Co0.1Mn0.1O2 cathode by tantalum doping

被引:0
|
作者
Cao, Bokai [1 ,2 ,3 ]
Fang, Hai-Tao [2 ]
Li, De [3 ]
Chen, Yong [1 ,3 ]
机构
[1] Foshan Univ, Sch Mat Sci & Hydrogen Energy, Guangdong Key Lab Hydrogen Energy Technol, Foshan 528000, Peoples R China
[2] Harbin Inst Technol, Sch Mat Sci & Engn, 92 West Dazhi St, Harbin 150001, Peoples R China
[3] Hainan Univ, State Key Lab Marine Resource Utilizat South China, Hainan Prov Key Lab Res Utilizat Si Zr Ti Resource, 58 Renmin Rd, Haikou 570228, Peoples R China
基金
中国国家自然科学基金;
关键词
D O I
10.1039/d4ta04307c
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The utilization of nickel-rich single-crystalline LiNi1-x-yCoxMnyO2 cathodes at elevated voltages encounters hindrances stemming from crack formation within micron-sized particles. While reducing particle dimensions offers a potential strategy to mitigate stress-induced cracking, it simultaneously exacerbates surface side reactions. Ta doping is presented to address these challenges, a Ta-doped single-crystalline LiNi0.8Co0.1Mn0.1O2 (Ta-SC) is engineered, integrating advantages of grain refinement and surface stability. Ta doping inhibits the growth of single crystals during sintering and suppresses the irreversible surface phase transition during cycling. Unlike the undoped SC cathode, which is susceptible to intragranular cracking, the Ta-SC cathode demonstrates excellent structural integrity upon high voltage cycling. This preservation of structural integrity in the Ta-SC cathode is attributed to homogeneous H2-H3 phase transition favoured by reduced kinetic barriers and short distance for Li+ diffusion. Benefitting from the structural stability, the Ta-SC cathode provides superior cycling stability. It maintains a coin cell capacity of 180.7 mA h g(-1) and retains an energy density of 679.8 W h kg(-1) after 200 cycles in the 2.8-4.8 V range at 1 C. This work highlights the potential of Ta doping as a general approach to improve the durability and electrochemical performance of layered cathode materials.
引用
收藏
页码:28363 / 28373
页数:11
相关论文
共 50 条
  • [1] Stabilizing the high-voltage cycle performance of LiNi0.8Co0.1Mn0.1O2 cathode material by Mg doping
    Liu, Xiaolan
    Wang, Shuo
    Wang, Li
    Wang, Ke
    Wu, Xiaozhong
    Zhou, Pengfei
    Miao, Zhichao
    Zhou, Jin
    Zhao, Yi
    Zhuo, Shuping
    JOURNAL OF POWER SOURCES, 2019, 438
  • [2] Nb-doping in LiNi0.8Co0.1Mn0.1O2 cathode material: Effect on the cycling stability and voltage decay at high rates
    Lei, Yike
    Ai, Jinjin
    Yang, Shuai
    Lai, Chunyan
    Xu, Qunjie
    JOURNAL OF THE TAIWAN INSTITUTE OF CHEMICAL ENGINEERS, 2019, 97 : 255 - 263
  • [3] Improved cycling stability of Ni-rich LiNi0.8Co0.1Mn0.1O2 cathode materials by optimizing Ti doping
    Wang, Nengneng
    Zhu, Yutao
    Yao, Jinlei
    Zhao, Meng
    Xu, Yanhui
    FUNCTIONAL MATERIALS LETTERS, 2021, 14 (01)
  • [4] Stable Molten Salts Mediated Growth of Single-Crystalline LiNi0.8Co0.1Mn0.1O2 with High Voltage Tolerance
    Zhang, Tao
    Qin, Zuoyu
    Long, Xiang
    Gao, Yuanhang
    Qin, Zuosu
    Zhang, Ning
    Guan, Cao
    Chen, Gen
    ADVANCED FUNCTIONAL MATERIALS, 2025,
  • [5] Self-Reconstruction of Highly Degraded LiNi0.8Co0.1Mn0.1O2 toward Stable Single-Crystalline Cathode
    Qin, Zuoyu
    Zhang, Tao
    Gao, Xuesong
    Luo, Wuqing
    Han, Junwei
    Lu, Bingan
    Zhou, Jiang
    Chen, Gen
    ADVANCED MATERIALS, 2024, 36 (05)
  • [6] Enhancing the High-Voltage Cycling Performance and Rate Capability of LiNi0.8Co0.1Mn0.1O2 Cathode Material by Codoping with Na and Br
    Zhang, Jiandong
    Wu, Fuzhong
    Dai, Xinyi
    Mai, Yi
    Gu, Yijing
    ACS SUSTAINABLE CHEMISTRY & ENGINEERING, 2021, 9 (04): : 1741 - 1753
  • [7] Improving the single crystal LiNi0.8Co0.1Mn0.1O2 cathode material performance by fluorine doping
    Zhang, Pengfei
    Liu, Zhaofeng
    Ma, Ben
    Li, Ping
    Zhou, Yingke
    Tian, Xiaohui
    CERAMICS INTERNATIONAL, 2021, 47 (23) : 33843 - 33852
  • [8] Impact of Surface Layer Formation during Cycling on the Thermal Stability of the LiNi0.8Co0.1Mn0.1O2 Cathode
    Komagata, Shogo
    Itou, Yuichi
    Kondo, Hiroki
    ACS APPLIED MATERIALS & INTERFACES, 2022, 14 (07) : 8931 - 8937
  • [9] Improving the cycling stability of LiNi0.8Co0.1Mn0.1O2 by boron doping to inhibit Li/Ni mixing
    Hu, Ziru
    Duan, Donghong
    Wang, Haorui
    Xu, Shoudong
    Chen, Liang
    Zhang, Ding
    CHEMICAL COMMUNICATIONS, 2023, 59 (83) : 12507 - 12510
  • [10] Optimization of the electrochemical properties of LiNi0.8Co0.1Mn0.1O2 cathode material by titanium doping
    Rui-Kai Yang
    Zhen-Guo Wu
    Yong-Chun Li
    Rong Li
    Lang Qiu
    Dong Wang
    Lin Yang
    Xiao-Dong Guo
    Ionics, 2020, 26 : 3223 - 3230