A unique microstructure and its formation mechanism induced by laser cladding of Ti6Al4V alloy produced by laser powder bed fusion

被引:2
|
作者
Liu, Yueyang [1 ]
Yang, Yang [1 ]
Chen, Chao [2 ]
机构
[1] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Peoples R China
[2] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
关键词
Pseudo-dendritic; Amorphous phase; New metastable phase; Homogeneous nucleation; Laser cladding; GLASS-FORMING ABILITY; WEAR-RESISTANCE; DIAGRAMS;
D O I
10.1016/j.jallcom.2024.174865
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A nickel based gradient laser cladding layer was successfully prepared on Ti6Al4V alloy produced by laser powder bed fusion (L-PBF). The nickel-enriched area of middle layer (NEAm) in the cladding layer had a unique structure. NEAm was composed of many large strip-like Ti2Ni grains. The sub-grain inside a single Ti2Ni grain presented a fine dendrite structure (these small dendrite units belong to the same grain, which was different from the traditional dendrite structure, so it was called "pseudo-dendrite"), the interdendrite was composed of amorphous phase or alternating beta-Ti, Ti5Si3 nano-grains or mixtures of amorphous phase and the alternating structure. There were many massive TiNi and dispersed Y2O3, TiC and other fine second phase particles in the dendrite stem. Some of the Si-rich amorphous phase in the interdendrite transformed into alternating beta-Ti and Ti5Si3 nano-grains. Thermodynamic calculation showed that the Gibbs free energies of amorphous phase in the top layer and NEAm were -13.353 and -33.619 kJ/mol, respectively. The glass-forming ability (GFA) values gamma(ABC)* of the top layer and NEAm were 1.813 and 3.067, respectively. Obviously, the amorphous phase formation was easier in the NEAm than in the top layer, which explains the reason that although the cooling rate in the NEAm is slower than that in the top layer, the amorphous phase is only generated in the NEAm. The two- dimensional mismatch between of Y2O3 and Ti2Ni reached 15.43%, which was larger than the limit value of heterogeneous nucleation (12%), so Y2O3 in the NEAm did not play a role in heterogeneous nucleation. An unreported metastable phase was identified in a grain of Y2O3 in the NEAm. Since this phase was sensitive to electron irradiation, extremely limited photo-information was acquired. Accordingly, the Bravais lattice of the metastable phase was reconstructed; its most likely structure was simple cubic. Its lattice constant was anew phase =3 root a(origin) (Y2O3) =1.8369 nm, alpha = beta = gamma = 90 degrees. Its orientational relationship with the parent-phase Y2O3 was {1 (1) over bar1} (origin Y2O3)parallel to{110} (new phase), <<(1)over bar>01>(origin Y2O3)parallel to;<<(1)over bar>10>(new phase). The large increase of the phase interface, the pinning effect of the second phase, and the formation of amorphous phase significantly increased the hardness(up to 1100HV).
引用
收藏
页数:15
相关论文
共 50 条
  • [1] SURFACE ROUGHNESS OF Ti6Al4V ALLOY PRODUCED BY LASER POWDER BED FUSION
    Liovic, David
    Franulovic, Marina
    Ferlic, Luka
    Gubeljak, Nenad
    FACTA UNIVERSITATIS-SERIES MECHANICAL ENGINEERING, 2024, 22 (01) : 63 - 76
  • [2] Microstructure and properties of Ni-Ti based gradient laser cladding layer of Ti6Al4V alloy by laser powder bed fusion
    Liu, Yueyang
    Yang, Yang
    Chen, Chao
    ADDITIVE MANUFACTURING, 2024, 79
  • [3] Qualification of Ti6Al4V ELI Alloy Produced by Laser Powder Bed Fusion for Biomedical Applications
    I. Yadroitsev
    P. Krakhmalev
    I. Yadroitsava
    A. Du Plessis
    JOM, 2018, 70 : 372 - 377
  • [4] Qualification of Ti6Al4V ELI Alloy Produced by Laser Powder Bed Fusion for Biomedical Applications
    Yadroitsev, I.
    Krakhmalev, P.
    Yadroitsava, I.
    Du Plessis, A.
    JOM, 2018, 70 (03) : 372 - 377
  • [5] Microstructure and Corrosion Resistance of Ti6Al4V Manufactured by Laser Powder Bed Fusion
    Luo, Yiwa
    Wang, Mingyong
    Zhu, Jun
    Tu, Jiguo
    Jiao, Shuqiang
    METALS, 2023, 13 (03)
  • [6] Characterization of Ti6Al4V Alloy Produced by Laser-Powder Bed Fusion and Surface Modification Using Nanosecond Laser
    Ribeiro, Gleicy de Lima Xavier
    de Castro, Renato Spacini
    dos Santos, Rogerio Goes
    Bugarin, Aline de Fatima Santos
    Terada, Maysa
    Batalha, Gilmar Ferreira
    Couto, Antonio
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2023, 26
  • [7] Influence of porosity on the fatigue life of laser powder bed fusion–produced Ti6Al4V
    Becker T.H.
    Dhansay N.M.
    Material Design and Processing Communications, 2021, 3 (01):
  • [8] High power laser powder bed fusion of Ti6Al4V alloy: The control of defects, microstructure, and mechanical properties
    Deng, Jinfeng
    Zhong, Qiao
    Chen, Jia
    Wei, Kaiwen
    Yue, Xiaoze
    Liu, Yuguang
    Li, Gaohang
    Li, Xiangyou
    Zeng, Xiaoyan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 4831 - 4843
  • [9] Study of the Effect of Nanosecond Laser Texturing on the Corrosion Behavior of Ti6Al4V and Ti6Al4V Parts Produced by Powder Bed Fusion
    Queiroz, Fernanda Martins
    Ribeiro, Gleicy de Lima Xavier
    de Castro, Renato Spacini
    dos Santos, Rogerio Goes
    Vieira, Alexandre
    Terada, Maysa
    Bugarin, Aline de Fatima Santos
    de Rossi, Wagner
    Costa, Isolda
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2023, 12 (03)
  • [10] A Review of the Fatigue Behaviour of Laser Powder Bed Fusion Ti6Al4V
    Moloi, Tumelo
    Dzogbewu, Thywill Cephas
    Maringa, Maina
    Muiruri, Amos
    METALLURGICAL & MATERIALS ENGINEERING, 2025, 31 (01) : 288 - 310