A new Ti-Al-Cr-Mo-Zr titanium alloy welding wire: Stability, microstructure and mechanical properties

被引:1
|
作者
Fang, Naiwen [1 ,2 ]
Wu, Pengbo [1 ,2 ]
Feng, Zhiqiang [1 ]
Wu, Bintao [2 ,3 ]
Luo, Jiutian [1 ]
Xu, Kai [2 ]
Li, Quan [1 ]
Xin, Guosong [4 ]
机构
[1] Beibu Gulf Univ, Qinzhou 535011, Peoples R China
[2] Harbin Welding Inst Ltd Co, Harbin 150028, Peoples R China
[3] Ningxia Univ, Yinchuan 750021, Peoples R China
[4] Juli New Mat Technol rizhao Co Ltd, Rizhao 276826, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 32卷
基金
中国国家自然科学基金;
关键词
Titanium alloy; Ti-Al-Cr-Zr welding wire; Microstructure and properties; HEAT-TREATMENT; GRAIN-REFINEMENT; ALPHA; METAL;
D O I
10.1016/j.jmrt.2024.07.162
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to improve the plasticity of titanium alloy welded joints, relevant scholars currently focus primarily on studying the mechanism of action of alloying elements Mo and V, such as reducing the phase transition temperature of the welded seam and ensuring a certain amount of (3 phase residue in the welded seam. In addition to improving the stability and strengthening ability of titanium alloy welded joint, it can also maintain a certain degree of plasticity of the welded joint. However, the poor impact toughness is still the key problem that restricts its long-term stable service in the harsh environment. Our work designed and developed a new Ti-Al-Cr-Mo-Zr solid welding wire, with the synergistic effect of Al, Cr, Mo and Zr, the welded seam microstructure and grain can be refined while ensuring the enough stiffness of the welding wire and its flatness during wire feeding into the designated working area. It ensures good wetting and spreading flow performance of the liquid molten pool metal in the welding process, so better welded seam formation can be obtained. The relative contents of alpha ' martensite and (3 phase in the welded seam are 76.79% and 23.21%, respectively. The residual (3 phase is interspersed between the alpha ' martensite of the slats. The (3 phase provides a path for the plastic deformation of the welded joint, making it easier for dislocation slip to pass the (3/alpha ' interface. At the same time, more dislocation slip channels and a small number of fine twins can be found in the interior of alpha ' martensite, which can ensure the strength while taking into account the toughness. After testing, it is found that the average tensile strength of welded joints is 901 MPa, which is close to 95% of the base metal (BM), the average post-fracture elongation of welded joints is 21%, and the impact toughness value at room temperature is distributed between 25 J and 33 J, which meets the requirements of the synergistic effect of welded joint strength and plastic toughness. It is suitable for long-term stable service of Ti64 titanium alloy welding structure under harsh working conditions.
引用
收藏
页码:23 / 36
页数:14
相关论文
共 50 条
  • [1] Microstructure and Properties of Laser Welded Joints of New Ti-Al-Cr-Mo-Zr Titanium Alloy Welding Wire
    Fang, Naiwen
    Feng, Zhiqiang
    Wu, Pengbo
    Huang, Ruisheng
    Luo, Jiutian
    Li, Quan
    Xin, Guosong
    RARE METAL MATERIALS AND ENGINEERING, 2025, 54 (01) : 147 - 155
  • [2] Microstructure and mechanical properties of wire arc additive repairing Ti-6.5Al-2Sn-2Zr-4Mo-4Cr titanium alloy
    Zhuo, Yimin
    Yang, Chunli
    Fan, Chenglei
    Lin, Sanbao
    Chen, Chao
    Cai, Xiaoyu
    MATERIALS SCIENCE AND TECHNOLOGY, 2020, 36 (15) : 1712 - 1719
  • [3] Microstructure and Mechanical Properties of Novel Ti-Al-V-Zr-Mo-Nb Cryogenic Titanium Alloy
    Lu Zichuan
    Sun Yachao
    Yao Caogen
    Li Shenggang
    Hou Zhimin
    Zhang Xuhu
    Ji Wei
    Zhang Haiyang
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (01) : 217 - 224
  • [4] Microstructure and Mechanical Properties of Novel Ti-Al-V-Zr-Mo-Nb Cryogenic Titanium Alloy
    Lu, Zichuan
    Sun, Yachao
    Yao, Caogen
    Li, Shenggang
    Hou, Zhimin
    Zhang, Xuhu
    Ji, Wei
    Zhang, Haiyang
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2022, 51 (01): : 217 - 224
  • [5] Microstructure and mechanical properties of powder metallurgy Ti-6Al-3Mo-1Zr titanium alloy
    Tan Y.
    Li N.
    Liu L.
    Zhang W.
    Yang C.
    Wang Z.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2024, 34 (05): : 1566 - 1578
  • [6] Microstructure and Mechanical Properties of Laser Welding Joint of Ti-6Al-2Zr-3Nb-Mo Alloy
    Liu, Jia
    Lei, Xiaowei
    Ma, Zhaowei
    Fu, Chengxue
    Fu, Zhanbo
    Du, Zhibo
    CHINESE JOURNAL OF LASERS-ZHONGGUO JIGUANG, 2022, 49 (16):
  • [7] Microstructure and mechanical properties of NiAl(Ti)-Cr(Mo) eutectic alloy
    Xiao Xuan
    Guo Jianting
    Yu Haipeng
    ACTA METALLURGICA SINICA, 2006, 42 (10) : 1031 - 1035
  • [8] Effect of inoculants Ti and Zr on microstructure and mechanical properties of 2219 Al-Cu alloy welding
    Yang, Chenggang
    Guo, Xuming
    Xing, Li
    Hanjie Xuebao/Transactions of the China Welding Institution, 2009, 30 (09): : 41 - 44
  • [9] Microstructure and Mechanical Properties of Hot Continuous Rolling Ti-Al-Nb-Zr-Mo Titanium Alloy Seamless Tube Welded by EBW
    Lv, Xueyan
    Wu, Shaojie
    Zhou, Xiaofeng
    Fan, Limin
    Feng, Jing
    Cheng, Fangjie
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2022, 51 (12): : 4376 - 4384