Effect of different surface treatments on the bonding potential and physical and mechanical properties of ultratranslucent zirconia

被引:1
|
作者
Abdulrahman, Doaa M. [1 ]
Sherief, Dalia I. [2 ]
El-Korashy, Dalia I. [2 ]
机构
[1] Ain Shams Univ, Fac Dent, Dent Biomat Dept, Org African Unity St El Qobba Bridge Al Waili, Cairo 11566, Egypt
[2] Ain Shams Univ, Fac Dent, Dent Biomat Biomat Dept, Cairo, Egypt
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2024年 / 132卷 / 01期
关键词
AIRBORNE-PARTICLE ABRASION; PHASE-TRANSFORMATION; FLEXURAL STRENGTH; RESIN CEMENT; ADHESION; HYDROPHILICITY; RESTORATIONS; TOPOGRAPHY; PRIMERS; PLASMA;
D O I
10.1016/j.prosdent.2022.06.002
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. Studies to determine a suitable surface treatment that improves bonding without compromising the strength or translucency of ultratranslucent zirconia are scarce. Purpose. The purpose of this in vitro study was to evaluate the effect of different surface treatments on translucency, surface topography, phase transformation, biaxial flexural strength, bond strength, and durability. Material and methods. A total of 169 ultratranslucent zirconia disks were randomly divided into 4 groups according to the surface treatment applied: airborne-particle abrasion (APA) (n=46), tribochemical silica airborne-particle abrasion (TS) (n=46), nonthermal oxygen plasma (NTP) (n=46), and no treatment, control (C) (n=31). The translucency parameter (Delta TP00) was evaluated with a spectrophotometer (n=15), phase transformation was assessed with an X-ray diffractometer (n=5), surface topography was evaluated with a scanning electron microscope (SEM) (n=3), and biaxial flexural strength (BFS) was tested with a universal testing machine (n=15). For the microshear bond strength (mu SBS) test, 40 composite resin specimens were attached to 8 disks and tested with a universal testing machine; 20 specimens were tested after 24 hours, and 20 specimens after hydrothermal aging in a thermocycler (TC). The data were analyzed with ANOVA followed by the Tukey post hoc test (alpha=.05). Weibull analysis was performed for the flexural strength and mu SBS results. Results. Significant Delta TP00 differences were found among all groups and were highest for the APA group (7.33) and lowest for the NTP group (4.79). The NTP group had a significantly higher monoclinic weight fraction value (4.54%) than other groups. The NTP group had significantly higher BFS (581.31) than other groups, while the APA group showed significantly lower values than other groups (340.43). The APA group had significantly higher mu SBS values after 24 hours (13.51 MPa) and after TC (13.68 MPa) than the other groups (P<.05). Conclusions. Although APA and TS are effective techniques for improving resin-zirconia bonding, they result in significantly higher deterioration of translucency and strength. NTP significantly improved the BFS of zirconia; however, it showed lower bond strength values than other methods.
引用
收藏
页码:219 / 228
页数:10
相关论文
共 50 条
  • [1] Mechanical Properties and Bonding Potential of Partially Stabilized Zirconia Treated with Different Chemomechanical Treatments
    EI-Korashy, Dalia I.
    Ei-Refai, Dina A.
    JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (04): : 365 - 376
  • [2] Mechanical properties of zirconia after different surface treatments and repeated firings
    Subasi, Meryem Gulce
    Demir, Necla
    Kara, Ozlem
    Ozturk, A. Nilgun
    Ozel, Faruk
    JOURNAL OF ADVANCED PROSTHODONTICS, 2014, 6 (06): : 462 - 467
  • [3] Effects of different plasma treatments on bonding properties of zirconia
    Jiang, Yulin
    Bao, Xudong
    Yu, Yang
    Zhang, Yannan
    Liu, Min
    Meng, Fanhao
    Wang, Bo
    Chen, Jianfeng
    HELIYON, 2024, 10 (12)
  • [4] Influence of surface treatments on highly translucent zirconia: Mechanical, optical properties and bonding performance
    Li, Xinyang
    Liang, Shengjie
    Li, Jing
    Tang, Wenhui
    Yu, Miaoyang
    Ahmed, Mohammed H.
    Liang, Shanshan
    Zhang, Fei
    Inokoshi, Masanao
    Yao, Chenmin
    Huang, Cui
    JOURNAL OF DENTISTRY, 2025, 154
  • [5] Zirconia Surface Treatments for Resin Bonding
    Cheung, George J. K.
    Botelho, Michael G.
    JOURNAL OF ADHESIVE DENTISTRY, 2015, 17 (06): : 551 - 558
  • [6] Effect of surface treatments on bonding strength of zirconia to dental cements
    Hashiguchi, M.
    Sato, H.
    Nishi, Y.
    Ban, S.
    Krnel, K.
    Kocjan, A.
    Kosmac, T.
    BIOCERAMICS 21, 2009, 396-398 : 575 - 578
  • [7] Surface Treatments of Zirconia to Enhance Bonding Durability
    Melo, R. M.
    Souza, R. O. A.
    Dursun, E.
    Monteiro, E. B. C.
    Valandro, L. F.
    Bottino, M. A.
    OPERATIVE DENTISTRY, 2015, 40 (06) : 636 - 643
  • [8] MORPHOLOGIC ANALYSIS OF ZIRCONIA CERAMICS: EFFECT OF DIFFERENT SURFACE TREATMENTS
    Chen, Chao
    Cao, Cong
    Yan, Xun
    Xu, Bao Hua
    INTERNATIONAL JOURNAL OF PERIODONTICS & RESTORATIVE DENTISTRY, 2023, 43 : S65 - S77
  • [9] Effect of Different Treatments on Waste Porcelain to the Physical and Mechanical Properties of Porcelain Production
    Salmi, Nur Hidayah
    Noh, Mohamad Zaky
    Sharip, Norazreen
    4TH INTERNATIONAL CONFERENCE ON THE SCIENCE AND ENGINEERING OF MATERIALS (ICOSEM 2019), 2020, 2284
  • [10] Effect of new zirconia surface coatings on the surface properties and bonding strength of veneering zirconia substrate
    Farhan, Firas Abdulameer
    Sulaiman, Eshamsul
    Kutty, Muralithran G.
    SURFACE & COATINGS TECHNOLOGY, 2018, 333 : 247 - 258