Effects of pre-strain deep cryogenic aging on the mechanical and corrosion properties of 2A97 aluminum-lithium alloy

被引:2
|
作者
Liu, Yan [1 ]
Zhao, Chenxu [1 ]
Chen, Junfeng [1 ]
Liu, Rongying [1 ]
Jiang, Jiantang [2 ]
Cui, Xiping [2 ]
Liang, Siyan [3 ]
Chi, Haitao [4 ]
Zou, Linchi [5 ]
机构
[1] Fuzhou Univ, Sch Mat Sci & Engn, Qishan Campus, Minhou 350116, Fujian, Peoples R China
[2] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 350001, Peoples R China
[3] Harbin Inst Technol Shenzhen, Sch Mat Sci & Engn, Shenzhen 518055, Peoples R China
[4] Fujian Xiangxin Light Alloys Manufacture Co Ltd, Fuzhou 350119, Peoples R China
[5] Fujian Univ Technol, Sch Mat Sci & Engn, Fuzhou 350118, Peoples R China
基金
中国国家自然科学基金;
关键词
Pre -strain deep cryogenic aging; Precipitate; Mechanical property; Corrosion property; LOCALIZED CORROSION; DEFORMATION-BEHAVIOR; PITTING CORROSION; T-1; PHASE; CU ALLOY; AL; PRECIPITATION; MICROSTRUCTURE; QUANTIFICATION; SUSCEPTIBILITY;
D O I
10.1016/j.jmrt.2024.03.213
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to improve the mechanical properties and corrosion resistance of 2A97 aluminum -lithium alloy, this research develops a novel strain heat -treatment technology. Surprisingly, 2A97 alloy treated by 4% pre -strain and 48 h deep cryogenic aging exhibits excellent mechanical properties, whose yield strength, tensile strength, and elongation are 573.7 MPa, 593.6 MPa, and 14.25%, respectively. Furthermore, the corrosion resistance of samples treated by the above pre -strain deep cryogenic aging process is two times as much as traditional T6 aged. This study deeply investigates the influence of various precipitates in 2A97 alloy on its performance through microstructure analysis. The results show that the introduction of pre -strain inhibits the precipitates of the T 1 and 8 ' phases at the grain boundaries, and prevents the formation and widening of precipitate -free zones. At the same time, it reduces the potential difference between grain boundaries and matrix, and enhances the corrosion resistance of 2A97 alloy. Deep cryogenic can inhibit recovery and maintain deformation dislocation, so that a large number of defects produced by pre -strain promote the nucleation and diffusion of precipitates in the matrix, resulting in tiny and uniformly distributed precipitates. Therefore, the novel prestrain deep cryogenic aging not only endues 2A97 alloy excellent performance, but also offers a new strategy for controlling precipitation.
引用
收藏
页码:2728 / 2737
页数:10
相关论文
共 50 条
  • [1] The Aging Behavior of Aluminum-Lithium Alloy 2A97
    Yuan Zhishan
    Wu Xiuliang
    Lu Zheng
    Xie Youhua
    Dai Shenglong
    Liu Changsheng
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 (11) : 1898 - 1902
  • [2] Effect of pre-strain on tensile mechanical properties of 2195 aluminum-lithium alloy
    Zhang Y.
    Ye L.
    Dong Y.
    Zou G.
    Li J.
    Yang X.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2024, 34 (03): : 725 - 738
  • [3] Study on Double-Aging of 2A97 Aluminum-Lithium Alloy
    Yuan Zhishan
    Lu Zheng
    Xie Youhua
    Wu Xiuliang
    Dai Shenglong
    Liu Changsheng
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (03) : 443 - 447
  • [4] Study on double-aging of 2A97 aluminum-lithium alloy
    Yuan, Zhishan
    Lu, Zheng
    Xie, Youhua
    Wu, Xiuliang
    Dai, Shenglong
    Liu, Changsheng
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2011, 40 (03): : 443 - 447
  • [5] Microstructure and mechanical properties of newly developed aluminum-lithium alloy 2A97 welded by fiber laser
    Fu, Banglong
    Qin, Guoliang
    Meng, Xiangmeng
    Ji, Yang
    Zou, Yong
    Lei, Zhen
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 617 : 1 - 11
  • [6] Effect of Aging Conditions on the Fatigue Crack Propagation Rate of 2A97 Aluminum-Lithium Alloy
    Xue Xili
    Zheng Ziqiao
    Hu Fang
    Zhang Long
    RARE METAL MATERIALS AND ENGINEERING, 2016, 45 (12) : 3319 - 3324
  • [7] Effects of intermediate annealing on grain refinement and superplasticity of 2A97 aluminum-lithium alloy
    Ye, Ling-Ying (30575421@qq.com), 2015, Central South University of Technology (25):
  • [8] Characterization of cryogenic mechanical properties of aluminum-lithium alloy C-458
    Vander Kooi, DC
    Park, W
    Hilton, MR
    SCRIPTA MATERIALIA, 1999, 41 (11) : 1185 - 1190
  • [9] Microstructure characterization and evaluation of mechanical properties in 2A97 aluminum-lithium alloys welded by stationary shoulder friction stir welding
    Sun, G. D.
    Zhou, L.
    Liu, Y. N.
    Yang, H. F.
    Jiang, J. T.
    Li, G. A.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 16 : 416 - 432
  • [10] Effects of pre-stretching on mechanical properties and corrosion behavior of superplastic formed 2A97 Al-Li alloy
    Xu, Yaqi
    Zou, Guotong
    Li, Jun
    Chen, Shijie
    Ye, Lingying
    MATERIALS CHARACTERIZATION, 2025, 222