Analysis of the Strength Property for TiC-Mo Composites at High Temperature

被引:3
|
作者
Shin, Soon-Gi [1 ]
机构
[1] Kangwon Natl Univ, Coll Samcheok, Dept Adv Mat Engn, Samcheok 245711, Gangwon, South Korea
来源
KOREAN JOURNAL OF MATERIALS RESEARCH | 2014年 / 24卷 / 04期
关键词
composites; high temperature; strength; compression test; rule of mixture;
D O I
10.3740/MRSK.2014.24.4.201
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
TiC-21 mol% Mo solid solution (delta-phase) and TiC-99 mol% Mo solid solution (beta-phase), and TiC-(80 similar to 90) mol% Mo hypo-eutectic composite were deformed by compression in a temperature range from room to 2300 K and in a strain rate range from 4.9 x 10(-5) to 6.9 x 10(-3)/s. The deformation behaviors of the composites were analyzed from the strengths of the delta- and beta-phases. It was found that the high strength of the eutectic composite is due primarily to solution hardening of TiC by Mo, and that the delta-phase undergoes an appreciable plastic deformation at and above 1420 K even at 0.2% plastic strain of the composite. The yield strength of the three kinds of phase up to 1420 K is quantitatively explained by the rule of mixture, where internal stresses introduced by plastic deformation are taken into account. Above 1420 K, however, the calculated yield strength was considerably larger than the measured strength. The yield stress of beta-phase was much larger than that of pure TiC. A good linear relationship was held between the yield stress and the plastic strain rate in a double-logarithmic plot. The deformation behavior in delta-phase was different among the three temperature ranges tested, i.e., low, intermediate and high. At an intermediate temperature, no yield drop occurred, and from the beginning the work hardening level was high. At the tested temperature, a good linear relationship was held in the double logarithmic plot of the yield stress against the plastic strain rate. The strain rate dependence of the yield stress was very weak up to 1273 K in the hypo-eutectic composite, but it became stronger as the temperature rose.
引用
收藏
页码:201 / 206
页数:6
相关论文
共 50 条
  • [1] Deformation Property of TiC-Mo Solid Solution Single Crystal at High Temperature by Compression Test
    Shin, Soon-Gi
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2014, 24 (11): : 625 - 631
  • [2] RETRACTED: Deformation Behavior of TiC-Mo Composites at High Temperature by Compression Test (Retracted Article)
    Shin, Soon-Gi
    KOREAN JOURNAL OF METALS AND MATERIALS, 2013, 51 (12): : 921 - 928
  • [3] Deformation Properties of TiC-Mo Eutectic Composite at High
    Shin, Soon-Gi
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2013, 23 (10): : 568 - 573
  • [4] Microstructure and Tribological Property of TiC-Mo Composite Coating Prepared by Vacuum Plasma Spraying
    Guo, Xiaoqian
    Niu, Yaran
    Huang, Liping
    Ji, Heng
    Zheng, Xuebin
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2012, 21 (05) : 1083 - 1090
  • [5] Microstructure and Tribological Property of TiC-Mo Composite Coating Prepared by Vacuum Plasma Spraying
    Xiaoqian Guo
    Yaran Niu
    Liping Huang
    Heng Ji
    Xuebin Zheng
    Journal of Thermal Spray Technology, 2012, 21 : 1083 - 1090
  • [6] Effect of Zr, Mo and TiC on microstructure and high-temperature tensile strength of cast titanium matrix composites
    Qi, J. Q.
    Chang, Y.
    He, Y. Z.
    Sui, Y. W.
    Wei, F. X.
    Meng, Q. K.
    Wei, Z. J.
    MATERIALS & DESIGN, 2016, 99 : 421 - 426
  • [7] MEASUREMENT AND ANALYSIS OF THE STRENGTH OF MO-TIC COMPOSITES IN THE TEMPERATURE-RANGE 285-K-2270-K
    KURISHITA, H
    SHIRAISHI, J
    MATSUBARA, R
    YOSHINAGA, H
    TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1987, 28 (01): : 20 - 31
  • [8] MEASUREMENT AND ANALYSIS OF THE STRENGTH OF MO-TIC COMPOSITES IN THE TEMPERATURE-RANGE 285 K-2270 K
    KURISHITA, H
    SHIRAISHI, J
    MATSUBARA, R
    YOSHINAGA, H
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1985, 49 (11) : 963 - 971
  • [9] High temperature strength of Mo/PSZ composites as evaluated by MSP test (II)
    Jiang, W
    Bai, GZ
    Wang, G
    Li, JF
    JOURNAL OF INORGANIC MATERIALS, 2002, 17 (05) : 1034 - 1040
  • [10] Structure of wear resistant coatings TiC-Mo, received electric-explosive spraying
    Romanov, D. A.
    Olesyuk, O. V.
    Budovskikh, E. A.
    Vaschuk, E. S.
    Gromov, V. E.
    OBRABOTKA METALLOV-METAL WORKING AND MATERIAL SCIENCE, 2013, (03): : 90 - 93