INVESTIGATION OF THE WEAR BEHAVIOR OF TYRE STEEL CORDS USING ELECTROCHEMICAL METHODS

被引:1
|
作者
REISENBAUER, A [1 ]
GRUNBERGER, A [1 ]
FEDERSPIEL, P [1 ]
NAUER, GE [1 ]
机构
[1] UNIV VIENNA,INST PHYS CHEM,WAHRINGERSTR 42,A-1090 VIENNA,AUSTRIA
关键词
Butler Volmer technique - Corrosion current density - Corrosion potential - Potassium sulfate - Tire steel cords;
D O I
10.1016/0043-1648(93)90372-S
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The goal of our investigations was to characterize tyre steel cords of different constructions according to their wear behaviour by measuring some corrosion parameters in dilute K2SO4 as electrolyte. The wear tests were performed using Hunter-type machines, where the probes with a length of 29.6 cm are fixed at one end by a guide hole and the other end is placed in a drilling jig. This drilling jig rotates with a definite velocity for different times (from 1 to 24 h). The effect of the fatigue on the corrosion behaviour of the steel cords was measured on single filaments of the same cords. During the rotation the cord filaments show characteristic wear damage, which can be measured using electrochemical techniques, such as the determination of the time dependence of the corrosion potential and of the corrosion current densities (using modified Butler-Volmer techniques). It was possible to show that the wear damage of steel cords depends strongly on the surrounding atmosphere during the Hunter treatment and on the construction of the steel cords. In an air or oxygen-containing atmosphere the cathodic reaction of the overall corrosion process is oxygen reduction. According to the large area of exposed surface, where oxygen reduction can proceed, the total corrosion reaction rate is high and, in relatively short times, visible corrosion products appear on some parts of the steel cord with wear damage of single filaments. We found highly negative corrosion potentials in relation to the untreated reference materials. In an argon atmosphere the corrosion reaction proceeds more slowly and we found more positive corrosion potentials, only small corrosion current densities and no significant wear damage.
引用
收藏
页码:57 / 62
页数:6
相关论文
共 50 条
  • [1] Wear mechanism of tungsten carbide dies during wet drawing of steel tyre cords
    Hollinger, S
    Depraetere, E
    Giroux, O
    WEAR, 2003, 255 (7-12) : 1291 - 1299
  • [2] Mechanical properties of SFRC using blended Recycled Tyre Steel Cords (RTSC) and Recycled Tyre Steel Fibres (RTSF)
    Hu, Hang
    Papastergiou, Panos
    Angelakopoulos, Harris
    Guadagnini, Maurizio
    Pilakoutas, Kypros
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 187 : 553 - 564
  • [3] An investigation on the corrosion of brass-coated steel cords for tyres by electrochemical techniques
    Chanel, S
    Pébère, N
    CORROSION SCIENCE, 2001, 43 (03) : 413 - 427
  • [4] Wear measurements using electrochemical methods
    Deforge, Damien
    Lina, Agnes
    Boursier, Jean-Marie
    Wenger, Francois
    Ponthiaux, Pierre
    Ambard, Antoine
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE 2005, VOL 4, 2005, 4 : 501 - 508
  • [5] STUDY OF POSSIBLE METHODS OF IMPROVING MODULUS OF NYLON 6.6 TYRE CORDS
    KENYON, D
    TEXTILE INSTITUTE AND INDUSTRY, 1968, 6 (09): : 234 - &
  • [7] Effect of sulfate ions on the corrosion behavior of steel in concrete using electrochemical methods
    Shi, Jinjie
    Sun, Wei
    ADVANCES IN STRUCTURES, PTS 1-5, 2011, 163-167 : 3049 - 3054
  • [8] Sensitivity analysis of the tyre design parameters with respect to tyre wear using a physical tyre model
    Braghin, F
    Cheli, F
    Melzi, S
    Resta, R
    VEHICLE SYSTEM DYNAMICS, 2005, 43 (SUPPL.) : 102 - 112
  • [9] Masonry Confinement Using Steel Cords
    Borri, Antonio
    Castori, Giulio
    Corradi, Marco
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2013, 25 (12) : 1910 - 1919
  • [10] METHODS OF INVESTIGATION OF EFFECT OF COMPRESSIVE STRESS ON WEAR-RESISTANCE OF STEEL
    KARABEKOV, MM
    KOLEV, KS
    INDUSTRIAL LABORATORY, 1976, 42 (03): : 444 - 446