INVESTIGATIONS OF THE HARDNESS AND THERMAL-PROPERTIES OF COPOLY(ETHER-ESTER)S CONTAINING SEGMENTS OF DIFFERENT MOLECULAR-WEIGHTS

被引:18
|
作者
SLONECKI, J
机构
[1] Technical University of Szczecin, Institute of Chemical Technology, 70-310 Szczecin
关键词
copoly(ether-ester)s; hardness; oligooxyethylenediol; poly(butylene-terephthalate); polycondensation;
D O I
10.1016/0032-3861(90)90151-N
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Copoly(ether-ester)s (CPPE) consisting of alternately arranged oligooxyethylene (PEO) soft segments of molecular weights 400 to 6000 and tetramethylene-terephthalate (4GT) hard segments was studied. The content of soft segments of copoly(ether-ester)s obtained varied over a wide range. Differential scanning calorimetry and hardness measurements in the temperature range from -70 to +150°C were carried out. At temperatures close to the melting point a significant change in hardness of CPEE occurs. This does not occur in those elastomers for which the enthalpy of melting (Hm) of the soft segments approaches zero. © 1990.
引用
收藏
页码:1464 / 1466
页数:3
相关论文
共 22 条