Stress corrosion cracking behaviour of precipitation hardened stainless steels in high purity water environments

被引:4
|
作者
Gaona-Tiburcio, C [1 ]
Almeraya-Calderón, F [1 ]
Martínez-Villafañe, A [1 ]
Bautista-Margulis, R [1 ]
机构
[1] Ctr Adv Mat Res, Chihuahua, Mexico
关键词
stress; crack propagation; corrosion; stainless steel;
D O I
10.1108/00035590110365318
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The susceptibility of 17-4PH and 17-7PH stainless steels to stress corrosion cracking (SCC) is examined in the present investigation. The specimens were tested in the presence of NaCl and NaOH (20%) at 90 degreesC and various pH values. The evaluations were carried out using the CERT test, at a speed of 10(-6)s(-1) supplemented by anodic polarisation and electrochemical noise analysis. The main objective was to identify the conditions of both susceptibility and performance of these materials. Fractographic analyses revealed both ductile and brittle fractures. Also, the presence of intergranular cracks was a clear indication of a characteristic anodic dissolution of the material. Nevertheless, the main mechanism for stress corrosion crack propagation was hydrogen embrittlement. From the experimental results, it was concluded that electrochemical noise analysis is a reliable technique for the identification of crack nucleation and growth.
引用
收藏
页码:37 / 46
页数:10
相关论文
共 50 条
  • [21] MECHANISM OF STRESS CORROSION CRACKING IN STAINLESS STEELS
    STICKLER, R
    BARNARTT, S
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1962, 109 (04) : 343 - 344
  • [22] MECHANISM OF STRESS CORROSION CRACKING IN STAINLESS STEELS
    SCULLY, JC
    STICKLER, R
    BARNARTT, S
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1962, 109 (12) : 1218 - 1219
  • [23] Behaviour of Stress Corrosion Cracking of Austenitic Stainless Steels in Sodium Chloride Solutions
    Elsariti, Samir Milad
    Haftirman
    MALAYSIAN TECHNICAL UNIVERSITIES CONFERENCE ON ENGINEERING & TECHNOLOGY 2012 (MUCET 2012), 2013, 53 : 650 - 654
  • [24] STRESS CORROSION CRACKING RESISTANCE OF COMMERCIAL AUSTENITIC STAINLESS STEELS IN HIGH TEMPERATURE WATER.
    Kowaka, Masamichi
    Kobayashi, Taiki
    Kudo, Takeo
    Sumitomo Metals, 1978, 30 (01): : 93 - 101
  • [25] Comparison of stress corrosion cracking of high-chromium stainless steels
    Qi, Yameng
    Zhang, Zhonghua
    Zhang, Chunxia
    JPT, Journal of Petroleum Technology, 2021, 73 (07): : 53 - 54
  • [26] Stress corrosion cracking of stainless steels in high temperature caustic solutions
    Rondelli, G
    Vicentini, B
    Sivieri, E
    CORROSION SCIENCE, 1997, 39 (06) : 1037 - 1049
  • [27] Hot cracking behaviour and susceptibility of extra high purity type 310 stainless steels
    Saida, K.
    Okabe, Y.
    Hata, K.
    Nishimoto, K.
    Kiuchi, K.
    Nakayama, J.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2010, 15 (01) : 87 - 96
  • [28] STRESS-CORROSION CRACKING BEHAVIOR OF MARTENSITIC STAINLESS-STEELS UNDER STATIC LOAD IN HIGH-TEMPERATURE HIGH-PURITY WATER
    OZAKI, T
    ISHIKAWA, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1989, 75 (08): : 1338 - 1345
  • [29] Influence of carbide precipitation and rolling direction on intergranular stress corrosion cracking of austenitic stainless steels in hydrogenated high-temperature water
    Arioka, K.
    Yamada, T.
    Terachi, T.
    Chiba, G.
    CORROSION, 2006, 62 (07) : 568 - 575
  • [30] Stress corrosion cracking susceptibility of austenitic stainless steels in supercritical water conditions
    Novotny, R.
    Hahner, P.
    Siegl, J.
    Hausild, P.
    Ripplinger, S.
    Penttila, S.
    Toivonen, A.
    JOURNAL OF NUCLEAR MATERIALS, 2011, 409 (02) : 117 - 123