ZrB2-SiC laminated ceramic composites

被引:36
|
作者
Lu, Zhihui [1 ,2 ]
Jiang, Dongliang [1 ]
Zhang, Jingxian [1 ]
Lin, Qingling [1 ]
Huang, Zhengren [1 ]
机构
[1] Chinese Acad Sci, Shanghai Inst Ceram, State Key Lab High Performance Ceram & Superfine, Shanghai 200050, Peoples R China
[2] Chinese Acad Sci, Grad Univ, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
ZrB2-SiC; Mechanical properties; Laminated ceramic composites; DIBORIDE-SILICON CARBIDE; HIGH TEMPERATURE CERAMICS; MECHANICAL-PROPERTIES; ZIRCONIUM; OXIDATION; MICROSTRUCTURE;
D O I
10.1016/j.jeurceramsoc.2011.04.020
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The oxidation behavior for ZrB2-20 vol% SiC (ZS20) and ZrB2-30 vol% SiC (ZS30) ceramics at 1500 degrees C was evaluated by weight gain measurements and cross-sectional microstructure analysis. Based on the oxidation results, laminated ZrB2-30 vol% SiC (ZS30)/ZrB2-25 vol% SiC (ZS25)/ZrB2-30 vol% SiC (ZS30) symmetric structure with ZS30 as the outer layer were prepared. The influence of thermal residual stress and the layer thickness ratio of outer and inner layer on the mechanical properties of ZS30/ZS25/ZS30 composites were studied. It was found that higher surface compressive stress resulted in higher flexural strength. The fracture toughness of ZS30/ZS25/ZS30 laminates was found to reach to 10.73 MPa m(1/2) at the layer thickness ratio of 0.5, which was almost 2 times that of ZS30 monolithic ceramics. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1435 / 1439
页数:5
相关论文
共 50 条
  • [21] Fracture toughness and R-curve behavior of laminated ZrB2-SiC/SiCw ceramic
    Li, Sujuan
    Wei, Chuncheng
    Wang, Weiwei
    Wang, Peng
    Liu, Yuying
    Li, Shuang
    Wen, Guangwu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 784 : 96 - 101
  • [22] Formation Mechanism of Zircon Phase in ZrB2-SiC Ceramic Composites during Oxidation
    Gao Dong
    Zhang Yue
    Xu Chun-Lai
    Song Yang
    Shi Xiao-Bin
    JOURNAL OF INORGANIC MATERIALS, 2011, 26 (04) : 433 - 437
  • [23] Fabrication of ZrB2-SiC ceramic composites by optimized gel-casting method
    Hong, Wenhu
    Hu, Ping
    Zhang, Dongyang
    Xie, Maosong
    Yang, Yang
    Du, Shanyi
    CERAMICS INTERNATIONAL, 2018, 44 (06) : 6037 - 6043
  • [24] Oxidation behaviour of laminated BN/ZrB2-SiC ceramics
    Liu, Xinchao
    Wei, Chuncheng
    Ji, Wenyi
    Li, Shuang
    Wang, Peng
    Zhou, Lijuan
    CERAMICS INTERNATIONAL, 2018, 44 (07) : 8374 - 8379
  • [25] The influence of ZrB2-SiC powders mechanical treatment on the structure of sintered ceramic composites
    Buyakova, S.
    Burlachenko, A.
    Mirovoi, Yu
    Sevostiyanova, I.
    Kulkov, S.
    INTERNATIONAL SEMINAR ON INTERDISCIPLINARY PROBLEMS IN ADDITIVE TECHNOLOGIES, 2016, 140
  • [26] Research progress of ZrB2-SiC ceramic coating on graphite and C/C composites
    Wang, Kai-Kai
    Li, Zheng-Xian
    Wang, Xin
    Li, Wei
    Xiang, Yuan-Fan
    Surface Technology, 2020, 49 (01): : 103 - 112
  • [27] Mechanical properties of ZrB2-SiC ceramic composites: room temperature instantaneous behaviour
    Orlovskaya, N.
    Stadelmann, R.
    Lugovy, M.
    Subbotin, V.
    Subhash, G.
    Neubert, M.
    Aneziris, C. G.
    Graule, T.
    Kuebler, J.
    ADVANCES IN APPLIED CERAMICS, 2013, 112 (01) : 9 - 16
  • [28] Oxidation of ZrB2-SiC Ultrahigh-Temperature Ceramic Composites in Dissociated Air
    Marschall, Jochen
    Pejakovic, Dusan A.
    Fahrenholtz, William G.
    Hilmas, Greg E.
    Zhu, Sumin
    Ridge, Jerry
    Fletcher, Douglas G.
    Asma, Cem O.
    Thomel, Jan
    JOURNAL OF THERMOPHYSICS AND HEAT TRANSFER, 2009, 23 (02) : 267 - 278
  • [29] Preparation of ZrB2-SiC ceramic composites and testing of its resistance to thermal shock
    Laboratory of Special Ceramics and Powder Metallurgy, University of Science and Technology Beijing, Beijing 100083, China
    Fenmo Yejin Jishu, 2008, 4 (260-264):
  • [30] Oxidation kinetics of hot-pressed ZrB2-SiC ceramic matrix composites
    Gao, Dong
    Zhang, Yue
    Xu, Chunlai
    Song, Yang
    Shi, Xiaobin
    CERAMICS INTERNATIONAL, 2013, 39 (03) : 3113 - 3119