Microstructure evolution and coarsening behavior of precipitated O phase in Ti-22Al-24Nb-0.5Mo (at. %) alloy during the heat treatment

被引:4
|
作者
Zhou, Xuan [1 ]
Liu, Jie [2 ]
Zhang, Shunmeng [1 ]
Fu, Li [1 ]
Cheng, Jun [3 ]
He, Junjie [1 ]
Xiong, Kai [1 ]
Li, Xin [2 ]
Lu, Shiqiang [2 ]
Mao, Yong [1 ]
Wang, Kelu [2 ]
机构
[1] Yunnan Univ, Mat Genome Inst, Sch Mat & Energy, Kunming 650091, Peoples R China
[2] Nanchang Hangkong Univ, Sch Aeronaut Mfg Engn, Nanchang 30063, Peoples R China
[3] Northwest Inst Nonferrous Met Res, Shaanxi Key Lab Biomed Met Mat, Xian 710016, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti-22Al-24Nb-0.5Mo alloy; Microstructure; Heat treatment; O phase; Coarsening behavior; TI2ALNB BASED ALLOY; TENSILE BEHAVIOR; LAMELLAR O; DEFORMATION MECHANISMS; CREEP RESISTANCE; HOT DEFORMATION; TI-22AL-25NB; MO; TI-6AL-4V; HARDNESS;
D O I
10.1016/j.jmrt.2023.10.197
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microstructure evolution and coarsening behavior of precipitated O phase were systematically investigated in this study, and the corresponding microstructures were characterized by scanning electron microscopy and transmission electron microscopy. The results showed that the original microstructure was composed of lath O phase, alpha 2 phase and B2 matrix. The precipitated O phase presented different morphologies and sizes during heat treatment. With the increase of solution temperature and holding time, the O phase occurred coarsening, with a thickness ranging from 0.73 increased to 2.64 mu m. But the volume fraction decreased from 57.65 to 18.40 %. During aging treatment, large amounts of fine secondary acicular O phase have precipitated from the matrix. As the aging temperature increases, the O phase underwent coarsening and the thickness increases from 0.70 to 1.40 mu m. However, the aging temperature has little effect on the precipitation of acicular O phase, and the volume fraction decreases from 37.66 to 33.32 %. Research found that the small-sized O phase gradually dissolved in the matrix, while the large-sized O phase grew. This phenomenon can be explained by Ostwald ripening mechanism. The TEM analysis revealed that the O phase occurred separation, mainly due to the diffusion of solute atoms and the embedding of B2 matrix. Meanwhile, the O phase had been completed and segmented. The coarsening mechanism of the O phase was also explained by the boundary splitting mechanism and terminal migration mechanism.
引用
收藏
页码:4236 / 4247
页数:12
相关论文
共 50 条
  • [21] Effect of hydrogenation on the microstructure of Ti-24Al-14Nb-3V-0.5Mo alloy
    Dong, L.
    Zhou, L.G.
    Ding, H.
    Zhang, C.B.
    Acta Metallurgica Sinica (English Letters), 1999, 12 (06): : 1289 - 1294
  • [22] Ti-22Al-24Nb-0.5Mo合金电子束焊接接头的组织和性能
    陈玮
    陈志勇
    赵桐
    唐振云
    稀有金属材料与工程, 2017, 46(S1) (S1) : 31 - 35
  • [23] Microstructure control and mechanical properties from isothermal forging and heat treatment of Ti-22Al-25Nb (at.%) orthorhombic alloy
    Wang, Wei
    Zeng, Weidong
    Xue, Chen
    Liang, Xiaobo
    Zhang, Jianwei
    INTERMETALLICS, 2015, 56 : 79 - 86
  • [24] Microstructure coarsening behavior of Ti-17 alloy with equiaxed alpha during heat treatment
    Xu, Jianwei
    Zeng, Weidong
    Jia, Zhiqiang
    Sun, Xin
    Zhou, Jianhua
    Journal of Alloys and Compounds, 2015, 618 : 343 - 348
  • [25] Microstructure coarsening behavior of Ti-17 alloy with equiaxed alpha during heat treatment
    Xu, Jianwei
    Zeng, Weidong
    Jia, Zhiqiang
    Sun, Xin
    Zhou, Jianhua
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 618 : 343 - 348
  • [26] Precipitation Behavior of O Phase during Continuous Cooling of Ti-22Al-25Nb Alloy
    Li, Dong
    Zeng, Weidong
    Zhang, Fan
    Xu, Jianwei
    Ma, Xiong
    Liang, Xiaobo
    METALS, 2022, 12 (02)
  • [27] Microstructure evolution and mechanical behavior of Ti-22Al-23Nb-1Mo-1Zr alloy ring forging
    Liu S.
    Zhou Y.
    Li J.
    Cao J.
    Cai J.
    Huang X.
    Dai S.
    Cailiao Gongcheng/Journal of Materials Engineering, 2022, 50 (04): : 147 - 155
  • [28] Evolution of microstructure and microhardness of the weld simulated heat-affected zone of Ti-22Al-25Nb (at.%) alloy with continuous cooling rate
    Shao, Ling
    Wu, Sujun
    Zhao, Shaofan
    Ketkaew, Jittisa
    Zhao, Haitao
    Ye, Fan
    Schroers, Jan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 744 : 487 - 492
  • [29] A diagram of isothermal decomposition of the β-phase in Ti-22Al-26Nb-0.5Zr-0.4Mo alloy
    Demakov, S. L.
    Komolikova, E. M.
    Vodolazskii, F. V.
    Popov, A. A.
    MATERIALS SCIENCE, 2008, 44 (03) : 374 - 379
  • [30] A diagram of isothermal decomposition of the β-phase in Ti-22Al-26Nb-0.5Zr-0.4Mo alloy
    S. L. Demakov
    E. M. Komolikova
    F. V. Vodolazskii
    A. A. Popov
    Materials Science, 2008, 44 : 374 - 379