CORROSION OF COPPER PIPE BY FLOWING PURE WATER.

被引:0
|
作者
Torigoe, Yutaka
Ichino, Takahide
Nakano, Yoshinobu
机构
来源
Boshoku gijutsu | 1979年 / 28卷 / 06期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
页码:343 / 347
相关论文
共 50 条
  • [1] ACCELERATED CORROSION OF COPPER IN FLOWING PURE WATER CONTAMINATED WITH OXYGEN AND SULFIDE
    SYRETT, BC
    CORROSION, 1977, 33 (07) : 257 - 262
  • [2] CORROSION OF COPPER TUBES IN FRESH WATER.
    Yamauchi, Shigenori
    Sato, Shiro
    Boshoku gijutsu, 1981, 30 (08): : 469 - 477
  • [3] ON THE CORROSION OF COPPER IN PURE WATER
    ERIKSEN, TE
    NDALAMBA, P
    GRENTHE, I
    CORROSION SCIENCE, 1989, 29 (10) : 1241 - 1250
  • [4] CORROSION FATIGUE OF HIGH STRENGTH STEEL IN SEA FLOWING WATER.
    Jang, Soon-Shik
    Shoji, Tetsuo
    Takahashi, Hideaki
    Watanabe, Yutaka
    1600, (35):
  • [5] Oscillatory dynamics of the pitting corrosion of copper in sea water.
    Garcia, E
    Uruchurtu, J
    Genesca, J
    AFINIDAD, 1996, 53 (464) : 215 - 222
  • [6] Intergranular erosion corrosion of pure copper tube in flowing NaCl solution
    Wu, Lei
    Ma, Aili
    Zhang, Lianmin
    Zheng, Yugui
    CORROSION SCIENCE, 2022, 201
  • [7] HYDROGEN EVOLUTION IN CORROSION OF COPPER IN PURE WATER
    HULTQUIST, G
    CORROSION SCIENCE, 1995, 37 (10) : U5 - U5
  • [8] HYDROGEN EVOLUTION IN CORROSION OF COPPER IN PURE WATER
    HULTQUIST, G
    CORROSION SCIENCE, 1987, 27 (07) : 785 - 785
  • [9] Hydrogen evolution in corrosion of copper in pure water
    Hultquist, G
    CORROSION SCIENCE, 1996, 38 (02) : U12 - U12
  • [10] Hydrogen evolution in corrosion of copper in pure water
    Department of Physical Chemistry, Royal Institute of Technology, S-100 44 Stockholm, Sweden
    Corros. Sci., 6 (0X):